EUVIMEDAtrasti EUVIMED
Vergleichsstudie

Color and Translucency Stability of Conventional, Milled, and 3D-Printed Provisional Restorative Materials After Cigarette Smoke Exposure and Brushing

İzim Türker Kader, Berkman Albayrak, Elif Nur Köroğlu, Göksel Kader

The International Journal of Prosthodontics · 2025

DOI: 10.11607/ijp.9494 ↗

At a glance

Vergleichsstudie in The International Journal of Prosthodontics, 2025. Written by İzim Türker Kader and 3 co-authors. Major MEDLINE topics: Printing, Three-Dimensional, Smoke, Toothbrushing, Dental Materials.

SantraukaSubjectsBibliografiniai duomenysCiteRelated studies

Abstract (original language)

PURPOSE: To evaluate the color and translucency changes of conventional, milled, and 3D-printed provisional restorative materials (PRMs) after cigarette smoke exposure and brushing. MATERIALS AND METHODS: A total of 120 disc-shaped (Ø6 mm × 2 mm) specimens were fabricated from conventional (CN; TempSmart, GC), milled (ML; FusionCeram), and 3D-printed (PR; TempPRINT, GC) PRMs (n = 40 per material). Specimens were randomly divided into smoke-exposed (S) and control (C) groups (n = 20). After 20 days of exposure (20 cigarettes/day, 2-second puffs, 60-second intervals) or artificial saliva storage, specimens underwent brushing simulation (15 strokes/day) to form S-BR and C-BR subgroups. Color and translucency were measured at baseline (T0), post-exposure (T1), and post-brushing (T2) using a spectrophotometer. Color change (ΔE00), translucency change (ΔTP00), and translucency parameter (TP00) were calculated. Data were analyzed using two-way robust ANOVA (5% trimmed means) and Tukey post hoc test (α = 0.05). RESULTS: ML exhibited significantly lower ΔE00 values than CN and PR after cigarette smoke exposure (P < .001). Brushing reduced discoloration in all smoking groups, especially for ML (P < .05). PR showed the highest ΔTP00 values across groups, differing significantly only from ML (P = .008). ML consistently demonstrated the highest TP00 values across all groups (P < .001), indicating superior translucency retention. CONCLUSIONS: Cigarette smoke adversely affected the optical properties of PRMs, particularly in conventional and 3D-printed resins. Milled materials exhibited superior resistance to discoloration and translucency change. Although brushing did not completely reverse staining, it effectively reduced discoloration, particularly in milled materials.

Subjects

MeSH terms (MEDLINE)

Printing, Three-DimensionalSmokeToothbrushingDental MaterialsColorMaterials TestingSaliva, ArtificialHumansSpectrophotometryTime FactorsComposite ResinsSilicon Compounds

Substances

SmokeDental MaterialsSaliva, ArtificialComposite ResinsSilicon Compounds

Cite

APA

Türker Kader, İ., Albayrak, B., Köroğlu, E. N., & Kader, G. (2025). Color and Translucency Stability of Conventional, Milled, and 3D-Printed Provisional Restorative Materials After Cigarette Smoke Exposure and Brushing. The International Journal of Prosthodontics. https://doi.org/10.11607/ijp.9494

Vancouver

Türker Kader İ, Albayrak B, Köroğlu EN, Kader G. Color and Translucency Stability of Conventional, Milled, and 3D-Printed Provisional Restorative Materials After Cigarette Smoke Exposure and Brushing. The International Journal of Prosthodontics. 2025. doi:10.11607/ijp.9494

BibTeX
@article{TrkerKader2025,
  author = {Türker Kader, İzim and Albayrak, Berkman and Köroğlu, Elif Nur and Kader, Göksel},
  title = {Color and Translucency Stability of Conventional, Milled, and 3D-Printed Provisional Restorative Materials After Cigarette Smoke Exposure and Brushing},
  journal = {The International Journal of Prosthodontics},
  year = {2025},
  doi = {10.11607/ijp.9494}
}
Start for free →