Color and Translucency Stability of Conventional, Milled, and 3D-Printed Provisional Restorative Materials After Cigarette Smoke Exposure and Brushing
The International Journal of Prosthodontics · 2025
DOI: 10.11607/ijp.9494 ↗Kurz gefasst
Vergleichsstudie in der Zeitschrift The International Journal of Prosthodontics, 2025. Verfasst von İzim Türker Kader und 3 weiteren Autor:innen. Hauptthemen laut MEDLINE: Printing, Three-Dimensional, Smoke, Toothbrushing, Dental Materials.
Abstract (Originalsprache)
PURPOSE: To evaluate the color and translucency changes of conventional, milled, and 3D-printed provisional restorative materials (PRMs) after cigarette smoke exposure and brushing. MATERIALS AND METHODS: A total of 120 disc-shaped (Ø6 mm × 2 mm) specimens were fabricated from conventional (CN; TempSmart, GC), milled (ML; FusionCeram), and 3D-printed (PR; TempPRINT, GC) PRMs (n = 40 per material). Specimens were randomly divided into smoke-exposed (S) and control (C) groups (n = 20). After 20 days of exposure (20 cigarettes/day, 2-second puffs, 60-second intervals) or artificial saliva storage, specimens underwent brushing simulation (15 strokes/day) to form S-BR and C-BR subgroups. Color and translucency were measured at baseline (T0), post-exposure (T1), and post-brushing (T2) using a spectrophotometer. Color change (ΔE00), translucency change (ΔTP00), and translucency parameter (TP00) were calculated. Data were analyzed using two-way robust ANOVA (5% trimmed means) and Tukey post hoc test (α = 0.05). RESULTS: ML exhibited significantly lower ΔE00 values than CN and PR after cigarette smoke exposure (P < .001). Brushing reduced discoloration in all smoking groups, especially for ML (P < .05). PR showed the highest ΔTP00 values across groups, differing significantly only from ML (P = .008). ML consistently demonstrated the highest TP00 values across all groups (P < .001), indicating superior translucency retention. CONCLUSIONS: Cigarette smoke adversely affected the optical properties of PRMs, particularly in conventional and 3D-printed resins. Milled materials exhibited superior resistance to discoloration and translucency change. Although brushing did not completely reverse staining, it effectively reduced discoloration, particularly in milled materials.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Substanzen
Zitieren
APA
Türker Kader, İ., Albayrak, B., Köroğlu, E. N., & Kader, G. (2025). Color and Translucency Stability of Conventional, Milled, and 3D-Printed Provisional Restorative Materials After Cigarette Smoke Exposure and Brushing. The International Journal of Prosthodontics. https://doi.org/10.11607/ijp.9494
Vancouver
Türker Kader İ, Albayrak B, Köroğlu EN, Kader G. Color and Translucency Stability of Conventional, Milled, and 3D-Printed Provisional Restorative Materials After Cigarette Smoke Exposure and Brushing. The International Journal of Prosthodontics. 2025. doi:10.11607/ijp.9494
BibTeX
@article{TrkerKader2025,
author = {Türker Kader, İzim and Albayrak, Berkman and Köroğlu, Elif Nur and Kader, Göksel},
title = {Color and Translucency Stability of Conventional, Milled, and 3D-Printed Provisional Restorative Materials After Cigarette Smoke Exposure and Brushing},
journal = {The International Journal of Prosthodontics},
year = {2025},
doi = {10.11607/ijp.9494}
}
EUVIMED