Effect of hatch distance on porcelain bond strength of metal frameworks produced by selective laser melting
The Journal of Prosthetic Dentistry · 2025
DOI: 10.1016/j.prosdent.2025.05.035 ↗Kurz gefasst
Fachartikel in der Zeitschrift The Journal of Prosthetic Dentistry, 2025. Verfasst von Taygun Sezer und 4 weiteren Autor:innen. Beteiligte Einrichtung: Lecturer, Department of Prosthodontics, Faculty of Dentistry, Erciyes University, Kayseri, Turkey. Hauptthemen laut MEDLINE: Lasers, Dental Porcelain, Dental Bonding, Metal Ceramic Alloys. Die Arbeit nennt 41 Literaturangaben. Gefördert von: Erciyes Üniversitesi.
Abstract (Originalsprache)
STATEMENT OF PROBLEM: The hatch distance, which refers to the spacing between adjacent laser lines in the laser melting process, may influence the microstructure of the metal framework and, hence, the metal-ceramic bond strength. However, studies on the influence of hatch distance on metal-ceramic bond strength are lacking. PURPOSE: The purpose of this in vitro study was to investigate the porcelain bond strength of cobalt chromium frameworks fabricated using selective laser melting with hatch distances of 50 µm, 55 µm, and 60 µm. MATERIAL AND METHODS: Bar-shaped cobalt chromium frameworks were fabricated using selective laser melting with hatch distances of 50 µm (Group-50), 55 µm (Group-55), and 60 µm (Group-60). After porcelain application, the metal-ceramic bond strength was evaluated using a 3-point bend test according to the International Organization for Standardization (ISO) 9693-1 standard. After the 3-point bend test, elemental analysis was performed on both the metal and porcelain interfaces of 1 randomly selected specimen from each group, and the density of 1 metal framework from each group was determined using the Archimedes method. In addition, microstructural analysis was performed on 1 metal framework from each group using optical microscopy, while 1 porcelain-applied metal framework was analyzed using scanning electron microscopy. The metal-ceramic bond strength data were statistically analyzed using a 1-way analysis of variance (α=.05) RESULTS: Hatch distance significantly affected the metal-ceramic bond strength (P
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Substanzen
Autor:innen und Institutionen
- Lecturer, Department of Prosthodontics, Faculty of Dentistry, Erciyes University, Kayseri, Turkey.
- Associate Professor, Department of Prosthodontics, Faculty of Dentistry, Erciyes University, Kayseri, Turkey.
- Private Practice, Ortoperio Oral and Dental Health Polyclinic, Kayseri, Turkey. Electronic address: dt.mustafaayata@gmail.com.
- Research Assistant, Department of Metallurgical and Materials Engineering, Faculty of Engineering, Kocaeli University, Kocaeli, Turkey.
- Professor, Department of Metallurgical and Materials Engineering, Faculty of Engineering, Kocaeli University, Kocaeli, Turkey.
Förderung
- Erciyes Üniversitesi
Zitieren
APA
Sezer, T., Albayrak, H., Ayata, M., Yavuz, H. İ., & Yamanoğlu, R. (2025). Effect of hatch distance on porcelain bond strength of metal frameworks produced by selective laser melting. The Journal of Prosthetic Dentistry. https://doi.org/10.1016/j.prosdent.2025.05.035
Vancouver
Sezer T, Albayrak H, Ayata M, Yavuz Hİ, Yamanoğlu R. Effect of hatch distance on porcelain bond strength of metal frameworks produced by selective laser melting. The Journal of Prosthetic Dentistry. 2025. doi:10.1016/j.prosdent.2025.05.035
BibTeX
@article{Sezer2025,
author = {Sezer, Taygun and Albayrak, Haydar and Ayata, Mustafa and Yavuz, Hasan İsmail and Yamanoğlu, Rıdvan},
title = {Effect of hatch distance on porcelain bond strength of metal frameworks produced by selective laser melting},
journal = {The Journal of Prosthetic Dentistry},
year = {2025},
doi = {10.1016/j.prosdent.2025.05.035}
}
EUVIMED