Fachartikel in der Zeitschrift The Journal of Prosthetic Dentistry, 2025. Verfasst von Yanan Zhou und 3 weiteren Autor:innen. Beteiligte Einrichtung: Lecturer, School of Mechanical Engineering, Shandong University of Technology, Zibo, PR China. Hauptthemen laut MEDLINE: Dental Bonding, Metal Ceramic Alloys, Dental Porcelain, Chromium Alloys. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 22 Literaturangaben.
Abstract (Originalsprache)
STATEMENT OF PROBLEM: The selective laser melting (SLM) technique has been a promising method of fabricating Co-Cr metal-ceramic restorations; however, the lower metal-ceramic bond properties of SLM Co-Cr restorations have become a major issue in clinical use. PURPOSE: The purpose of this in vitro study was to propose and verify a method of improving the metal-ceramic bond properties of SLM Co-Cr alloy with heat treatment after porcelain firing (PH). MATERIAL AND METHODS: Forty-eight (25×3×0.5 mm) Co-Cr specimens, divided into 6 groups (Control group [CG]; 550 °C; 650 °C; 750 °C; 850 °C; 950 °C) according to PH temperatures, were prepared by using SLM techniques. The 3-point bend tests were performed to evaluate the metal-ceramic bond strengths; subsequently, the fracture feature was assessed by using a digital camera and scanning electron microscope (SEM) coupled with an energy-dispersive X-ray spectroscopy (EDS) detector, to determine the area fraction of adherence porcelain (AFAP). The interface morphologies and element distribution were determined with SEM/EDS detectors. Phase identification and quantification were examined with an X-ray diffractometer (XRD). A 1-way ANOVA and the Tukey honestly significant difference tests were used to analyze bond strengths and AFAP values (α=.05). RESULTS: The bond strengths were 35.33 ±1.25 MPa for the CG group, 34.53 ±3.20 MPa for the 550 °C group, 38.20 ±2.60 MPa for the 650 °C group, 42.85 ±2.31 MPa for the 750 °C group, 33.28 ±3.85 MPa for the 850 °C group, and 29.09 ±2.86 MPa for the 950 °C group. Significant differences were not observed among the CG, 550 °C, and 850 °C groups (P>.05) but were found among the other groups (P
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Substanzen
Autor:innen und Institutionen
- Lecturer, School of Mechanical Engineering, Shandong University of Technology, Zibo, PR China.
- Graduate student, School of Mechanical Engineering, Sichuan University, Chengdu, PR China.
- Professor, School of Mechanical Engineering, Sichuan University, Chengdu, PR China.
- Associate Professor, School of Mechanical Engineering, Sichuan University, Chengdu, PR China. Electronic address: yanjiazhen@scu.edu.cn.
Zitieren
APA
Zhou, Y., Dong, X., Li, N., & Yan, J. (2025). Effects of posttreatment on the metal-ceramic bond properties of selective-laser-melted Co-Cr dental alloy—Part 2: Heat treatment after porcelain firing. The Journal of Prosthetic Dentistry. https://doi.org/10.1016/j.prosdent.2023.01.030
Vancouver
Zhou Y, Dong X, Li N, Yan J. Effects of posttreatment on the metal-ceramic bond properties of selective-laser-melted Co-Cr dental alloy—Part 2: Heat treatment after porcelain firing. The Journal of Prosthetic Dentistry. 2025. doi:10.1016/j.prosdent.2023.01.030
BibTeX
@article{Zhou2025,
author = {Zhou, Yanan and Dong, Xin and Li, Ning and Yan, Jiazhen},
title = {Effects of posttreatment on the metal-ceramic bond properties of selective-laser-melted Co-Cr dental alloy—Part 2: Heat treatment after porcelain firing},
journal = {The Journal of Prosthetic Dentistry},
year = {2025},
doi = {10.1016/j.prosdent.2023.01.030}
}
EUVIMED