Comparative evaluation of postfabrication thickness of thermoformed 3 mm and 4 mm mouthguards on crowded and proclined malocclusion models: An in vitro study

Ritesh Kalaskar, Nidhi Sharma, Ashita Kalaskar

Journal of Indian Society of Pedodontics and Preventive Dentistry · 2026

DOI: 10.4103/jisppd.jisppd_389_26 ↗

Kurz gefasst

Vergleichsstudie in der Zeitschrift Journal of Indian Society of Pedodontics and Preventive Dentistry, 2026. Verfasst von Ritesh Kalaskar und 2 weiteren Autor:innen. Beteiligte Einrichtung: Department of Paediatric and Preventive Dentistry and Oral Medicine and Radiology, Government Dental College and Hospital, Nagpur, Maharashtra, India. Hauptthemen laut MEDLINE: Mouth Protectors, Malocclusion. Die Arbeit nennt 35 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Purpose

To evaluate and compare the postfabrication thickness (PFT) of thermoformed mouthguards fabricated from 3 mm and 4 mm ethylene-vinyl acetate (EVA) sheets on crowded and proclined dental models. Materials and Methods: An in-vitro study was conducted using 20 mouthguards fabricated on dental stone models with crowded and proclined maxillary anterior teeth. Pressure-molded mouthguards were made using 3 mm and 4 mm EVA sheets. PFT was measured at standardized labial, buccal, and sulcus regions using an Iwanson caliper. Statistical analysis was performed using ANOVA, Tukey’s post hoc test, and unpaired t -test ( P < 0.05).

Results

Significant thickness reduction was observed in both 3 mm and 4 mm mouthguards. In crowded dentition, 42%–61% thinning occurred at labial surfaces and 53%–71% at the sulcus, while proclined dentition showed 40%–60% and 51%–67% thinning, respectively. Maximum thinning occurred at canines, whereas molars showed the least reduction.

Conclusion

Thermoforming causes substantial reduction in mouthguard thickness, particularly in anterior regions. Dental alignment influences final thickness, and clinicians should consider postfabrication thinning when selecting EVA sheet thickness to ensure adequate protection.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

Mouth ProtectorsMalocclusionHumansModels, DentalIn Vitro TechniquesPolyvinylsEquipment DesignVinyl Compounds

Stichwörter der Autor:innen

Ethylene-vinyl acetatemalocclusionmouthguardsorofacial injurypostfabrication thicknessthermoforming

Substanzen

ethylenevinylacetate copolymerPolyvinylsVinyl Compounds

Autor:innen und Institutionen

  • Department of Paediatric and Preventive Dentistry and Oral Medicine and Radiology, Government Dental College and Hospital, Nagpur, Maharashtra, India.

Zitieren

APA

Kalaskar, R., Sharma, N., & Kalaskar, A. (2026). Comparative evaluation of postfabrication thickness of thermoformed 3 mm and 4 mm mouthguards on crowded and proclined malocclusion models: An in vitro study. Journal of Indian Society of Pedodontics and Preventive Dentistry. https://doi.org/10.4103/jisppd.jisppd_389_26

Vancouver

Kalaskar R, Sharma N, Kalaskar A. Comparative evaluation of postfabrication thickness of thermoformed 3 mm and 4 mm mouthguards on crowded and proclined malocclusion models: An in vitro study. Journal of Indian Society of Pedodontics and Preventive Dentistry. 2026. doi:10.4103/jisppd.jisppd_389_26

BibTeX
@article{Kalaskar2026,
  author = {Kalaskar, Ritesh and Sharma, Nidhi and Kalaskar, Ashita},
  title = {Comparative evaluation of postfabrication thickness of thermoformed 3 mm and 4 mm mouthguards on crowded and proclined malocclusion models: An in vitro study},
  journal = {Journal of Indian Society of Pedodontics and Preventive Dentistry},
  year = {2026},
  doi = {10.4103/jisppd.jisppd_389_26}
}
Kostenlos starten →