EUVIMEDEUVIMED entdecken
Crossref

Effects of heat treatment temperature and time on the fitness accuracy, retentive force, and permanent deformation of selective laser melting Ti-6Al-4V clasps

Lu-Xiang Yu, Na Yu, Jing-Jing Fan, Peng Wang, Lu Liu, Fa-Bing Tan

Materials Science in Additive Manufacturing · 12.03.2026 · 5 (2) · 025490118

DOI: 10.36922/msam025490118 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials Science in Additive Manufacturing, online erschienen am 12.03.2026. Verfasst von Lu-Xiang Yu und 5 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The selective laser melting (SLM) technology of Ti-6Al-4V (TC4) demonstrates significant advantages in fabricating clasps for removable partial dentures, whereas subsequent heat treatment plays a crucial role in performance optimization. This study systematically investigated the effects of heat treatment temperature and time on the fitness accuracy, retentive force, and permanent deformation of SLM TC4 clasps. TC4 clasp specimens were manufactured using SLM technology and subjected to heat treatment under different temperatures (700, 750, 800, and 850℃) and times (0.5, 1.0, and 1.5 h). The fitness accuracy, retentive force, and permanent deformation after 10,000 insertion/removal cycles were measured for each group and statistically analyzed. The results revealed that the 700℃/0.5 h group showed significantly reduced fitness accuracy. After cyclic testing, the retentive force of all groups decreased by 4.06%–12.18%, with heat treatment temperature significantly affecting both initial and final retentive forces. The time of heat treatment demonstrated no substantial influence. The permanent deformation of the clasps (31.15–38.05 μm) remained unaffected by variations in either heat treatment temperature or time. Based on overall performance, the 700℃/0.5 h heat treatment condition is not recommended. Instead, selecting shorter time protocols such as 0.5 h within the 750℃–850℃ range can help enhance production efficiency while maintaining performance standards.

Zitieren

APA

Yu, L., Yu, N., Fan, J., Wang, P., Liu, L., & Tan, F. (2026). Effects of heat treatment temperature and time on the fitness accuracy, retentive force, and permanent deformation of selective laser melting Ti-6Al-4V clasps. Materials Science in Additive Manufacturing, 5(2), 025490118. https://doi.org/10.36922/msam025490118

Vancouver

Yu L, Yu N, Fan J, Wang P, Liu L, Tan F. Effects of heat treatment temperature and time on the fitness accuracy, retentive force, and permanent deformation of selective laser melting Ti-6Al-4V clasps. Materials Science in Additive Manufacturing. 2026;5(2):025490118. doi:10.36922/msam025490118

BibTeX
@article{Yu2026,
  author = {Yu, Lu-Xiang and Yu, Na and Fan, Jing-Jing and Wang, Peng and Liu, Lu and Tan, Fa-Bing},
  title = {Effects of heat treatment temperature and time on the fitness accuracy, retentive force, and permanent deformation of selective laser melting Ti-6Al-4V clasps},
  journal = {Materials Science in Additive Manufacturing},
  year = {2026},
  volume = {5},
  number = {2},
  pages = {025490118},
  doi = {10.36922/msam025490118}
}
Kostenlos starten →