Microstructure and Mechanical Properties of LaB6/Ti-6Al-4V Composites Fabricated by Selective Laser Melting

Dongdong He, Hui Wang, Weidong Huang, Xinxi Chen, Guofu Lian, Yu Wang

Metals · 29.01.2023 · 13 (2) · 264

DOI: 10.3390/met13020264 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Metals, online erschienen am 29.01.2023. Verfasst von Dongdong He und 5 weiteren Autor:innen. Die Arbeit wurde bisher 22-mal zitiert (Crossref) und nennt 34 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: the National Natural Science Foundation of China, the Natural Science Foundation of Fujian Province, the Fujian Industry University Cooperation Project.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

In this study, TiB + La2O3/Ti-6Al-4V composites were successfully prepared by in situ reaction using selective laser melting technology. The effect of LaB6 content on the fabrication quality, microstructure evolution and mechanical properties of the composite samples was investigated. The results show that the relative density of the sample gradually decreased from 98.56% to 96.57% as LaB6 content increased from 0 wt% to 3 wt%. With increasing LaB6 content, TiB precipitates gradually aggregated and grew from a discrete needle-like structure to a dendritic structure, before eventually developing a cell-like structure. The dislocations piled up around the TiB and La2O3 reinforcements, which impeded the motion of the dislocations and led to the enhancement of the tensile strength of the samples. Different from the addition of a single reinforcement due to the combined strengthening effect of the micrometer-scale and nanoscale reinforcements, the strength of the samples was increased significantly. The Ti-6Al-4V sample with 3 wt% LaB6 addition showed the most significant strengthening effect. Compared to the pure Ti-6Al-4V sample, the 3 wt% LaB6 addition sample gained a 35.71% increase in hardness and a 14.5% increase in tensile strength. Additionally, wear volume was reduced by 47.5%. The results revealed that the addition of LaB6 was a potential way to improve the mechanical performance of the titanium alloys in the additive manufacturing process.

Förderung

  • the National Natural Science Foundation of China
  • the Natural Science Foundation of Fujian Province
  • the Fujian Industry University Cooperation Project
  • the Fujian Innovation Center of Additive Manufacturing

Zitieren

APA

He, D., Wang, H., Huang, W., Chen, X., Lian, G., & Wang, Y. (2023). Microstructure and Mechanical Properties of LaB6/Ti-6Al-4V Composites Fabricated by Selective Laser Melting. Metals, 13(2), 264. https://doi.org/10.3390/met13020264

Vancouver

He D, Wang H, Huang W, Chen X, Lian G, Wang Y. Microstructure and Mechanical Properties of LaB6/Ti-6Al-4V Composites Fabricated by Selective Laser Melting. Metals. 2023;13(2):264. doi:10.3390/met13020264

BibTeX
@article{He2023,
  author = {He, Dongdong and Wang, Hui and Huang, Weidong and Chen, Xinxi and Lian, Guofu and Wang, Yu},
  title = {Microstructure and Mechanical Properties of LaB6/Ti-6Al-4V Composites Fabricated by Selective Laser Melting},
  journal = {Metals},
  year = {2023},
  volume = {13},
  number = {2},
  pages = {264},
  doi = {10.3390/met13020264}
}
Kostenlos starten →