EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

The Microstructure and Properties of Al–Mn–Cu–Zr Alloy after High-Energy Ball Milling and Hot-Press Sintering

Olga A. Yakovtseva, Andrey G. Mochugovskiy, Alexey S. Prosviryakov, Andrey I. Bazlov, Nadezhda B. Emelina, Anastasia V. Mikhaylovskaya

Metals · 06.03.2024 · 14 (3) · 310

DOI: 10.3390/met14030310 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Metals, online erschienen am 06.03.2024. Verfasst von Olga A. Yakovtseva und 5 weiteren Autor:innen. Die Arbeit wurde bisher 16-mal zitiert (Crossref) und nennt 115 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Russian Science Foundation.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

In the present research an Al–7.7%Mn–4.9%Zr–3.2%Cu (wt%) alloy was processed by mechanical alloying (MA) followed by hot press sintering. The microstructure, phase composition, and mechanical properties of the MA granules and sintered samples were investigated. The dissolution of Mn, Zr, and Cu with further precipitation of the Al6Mn phase were observed during high-energy ball milling. In the alloy processed without stearic acid after milling for ~10 h, an Al-based solid solution with ~4.9 wt%Zr, ~3.2 wt%Cu and a ~5 wt%Mn with a grain size of ~16 nm and a microhardness of ~530 HV were observed. The addition of stearic acid facilitated Mn dissolution and precipitation of the Al6Mn phase during milling but led to the formation of the ZrH2 phase that decreased the Zr solute and the microhardness. Precipitation of the Al6Mn, L12–Al3Zr, and Al2Cu phases during annealing and sintering of the MA granules in the temperate range of 350–375 °C was observed, and an additional Al20Cu2Mn3 phase was precipitated at 400–450 °C. Hot-press sintering at 450 °C provided a low fraction of cavities of ~1.5%, the yield strength of 1100 MPa, ultimate compressive strength of 1200 MPa, strain at fracture of 0.5% at room temperature, the yield strength of 380 MPa, ultimate compressive strength of 440 MPa, and strain at fracture of 3.5% at 350 °C. The microstructural evolution during high-temperature deformation on the sample surface was studied and the differences in deformation behavior for the alloys sintered at different temperatures were discussed.

Förderung

  • Russian Science Foundation

Zitieren

APA

Yakovtseva, O. A., Mochugovskiy, A. G., Prosviryakov, A. S., Bazlov, A. I., Emelina, N. B., & Mikhaylovskaya, A. V. (2024). The Microstructure and Properties of Al–Mn–Cu–Zr Alloy after High-Energy Ball Milling and Hot-Press Sintering. Metals, 14(3), 310. https://doi.org/10.3390/met14030310

Vancouver

Yakovtseva OA, Mochugovskiy AG, Prosviryakov AS, Bazlov AI, Emelina NB, Mikhaylovskaya AV. The Microstructure and Properties of Al–Mn–Cu–Zr Alloy after High-Energy Ball Milling and Hot-Press Sintering. Metals. 2024;14(3):310. doi:10.3390/met14030310

BibTeX
@article{Yakovtseva2024,
  author = {Yakovtseva, Olga A. and Mochugovskiy, Andrey G. and Prosviryakov, Alexey S. and Bazlov, Andrey I. and Emelina, Nadezhda B. and Mikhaylovskaya, Anastasia V.},
  title = {The Microstructure and Properties of Al–Mn–Cu–Zr Alloy after High-Energy Ball Milling and Hot-Press Sintering},
  journal = {Metals},
  year = {2024},
  volume = {14},
  number = {3},
  pages = {310},
  doi = {10.3390/met14030310}
}
Kostenlos starten →