Background: The purpose of this in vitro study was to evaluate and compare the shear bond strength (SBS) and failure mode kinetics of indirect 3D-printed ceramic-reinforced hybrid composite restorations to human tooth dentin using fourth-generation etch-and-rinse and sixth-generation self-etch adhesive systems under a co-curing protocol with a preheated universal composite resin luting material.Methods and Results: Sound human third molars (N=156) were prepared to expose flat mid-dentin surfaces.Simulated indirect restorations were additively manufactured as composite cylinders (VarseoSmile TriniQ, BEGO) using a Formlabs Form 4B 3D printer.Samples were randomly divided into two experimental groups based on the adhesive system used: Group 1 (n=78, OptiBond FL, fourth generation) and Group 2 (n=78, Clearfil SE Bond 2, sixth generation).Preheated universal composite resin (Filtek Z350, 55°C) was used for luting under a co-curing sequence.Each group was subdivided (n=39) into a baseline subgroup (immediate testing) and a thermocycling subgroup (10,000 cycles, 5°C/55°C).SBS trials were performed at a crosshead speed of 1 mm/min, and debonded surfaces were evaluated under 40× magnification to classify failure modes.Statistical analysis was performed using SciPy 1.11.For continuous data with a normal distribution, inter-group comparisons were performed using Student's t-test.Categorical variables were analyzed using the chi-square test.A P-value 0.05) and identical mixed failure profiles.Thermocycling significantly degraded dentin bond integrity across all cohorts (P=0.000).However, post-aging evaluation revealed that Clearfil SE Bond 2 (16.8 ± 4.4 MPa) had a significantly higher remaining SBS than OptiBond FL (14.4 ± 4.7 MPa), P = 0.023.Microscopic analysis confirmed a complete absence of cohesive failures.Following thermal aging, the OptiBond FL interface underwent an acute intra-group shift toward true adhesive failures (84.6%), whereas Clearfil SE Bond 2 maintained high structural stability with a lower adhesive failure rate (61.5%),P= 0.022.Conclusion.While both adhesive strategies exhibit equivalent immediate performance during preheated composite co-curing, the null hypothesis must be rejected after artificial aging.The sixth-generation 10-MDP-containing self-etch system provides superior hydrolytic stability and interfacial durability compared to the fourth-generation system.Clinically, a two-step self-etch protocol provides a more predictable, chemically driven interface for the long-term cementation of contemporary additively manufactured restorations.(
Zitieren
APA
(2026). In Vitro Dentin Bond Durability of Additively Manufactured Hybrid Composite Restorations Luted with Preheated Composite: A Comparative Analysis of Fourth- and Sixth-Generation Adhesives. International Journal of Biomedicine, 16(2). https://doi.org/10.21103/article16(2)_oa14
Vancouver
In Vitro Dentin Bond Durability of Additively Manufactured Hybrid Composite Restorations Luted with Preheated Composite: A Comparative Analysis of Fourth- and Sixth-Generation Adhesives. International Journal of Biomedicine. 2026;16(2). doi:10.21103/article16(2)_oa14
BibTeX
@article{euvimed2026,
title = {In Vitro Dentin Bond Durability of Additively Manufactured Hybrid Composite Restorations Luted with Preheated Composite: A Comparative Analysis of Fourth- and Sixth-Generation Adhesives},
journal = {International Journal of Biomedicine},
year = {2026},
volume = {16},
number = {2},
doi = {10.21103/article16(2)_oa14}
}
EUVIMED