Performance and durability of additively and subtractively manufactured resin‐based onlay restorations after thermomechanical aging

Mehmet Esad Güven, Mustafa Borga Donmez, Ayyüce Nur Tezcan, Hyung-In Yoon, Burak Yilmaz iD, Gülce Çakmak

Journal of Prosthodontics · 18.12.2024

DOI: 10.1111/jopr.14005 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Prosthodontics, online erschienen am 18.12.2024. Verfasst von Mehmet Esad Güven und 5 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthodontics, Faculty of Dentistry, Necmettin Erbakan University, Konya, Turkey. Die Arbeit wurde bisher 7-mal zitiert (Crossref) und nennt 25 Literaturangaben. Gefördert von: Buser Implant Foundation Junior Investigator.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Purpose

To evaluate the effect of material type on dimensional stability, occlusal surface wear, fracture resistance, and failure behavior of resin‐based onlay restorations. Material and Methods A mandibular right first molar typodont was prepared and digitized using an intraoral scanner to virtually design an onlay restoration with the minimum occlusal thickness of 1.5 mm. Resin‐based onlay restorations ( n = 15 per group) were fabricated either additively from 2 different resins indicated either for definitive or interim use or subtractively with a composite resin. After cementing onlays to corresponding dies, each of them was digitized before and after thermomechanical aging (B‐STL and A‐STL), and then subjected to load‐to‐failure test to evaluate fracture resistance. The B‐STL and A‐STL of each onlay were also compared to assess the dimensional stability and occlusal surface wear. One‐way analysis of variance and Tukey honestly significant difference tests were used to evaluate dimensional stability, occlusal surface wear, and fracture resistance. The chi‐square test was used to evaluate the Weibull modulus and characteristic strength among the groups ( α = 0.05).

Results

Material type affected investigated outcomes ( p < 0.001). The additively manufactured resin indicated for definitive use led to the highest external surface deviations and the additively manufactured resin indicated for interim use led to the highest mesiodistal width deviations ( p ≤ 0.033). The onlays fabricated from the additively manufactured resin indicated for definitive use had the highest occlusal surface wear, while those in composite resin had the lowest ( p ≤ 0.006). The composite resin onlays had the highest fracture resistance values and reliability ( p ≤ 0.035).

Conclusions

Tested subtractively manufactured composite resin had the lowest occlusal surface wear with the highest fracture resistance and reliability. Additively manufactured resins had lower dimensional stability, while tested resin for additively manufactured definitive restorations had the highest occlusal surface wear.

Schlagwörter

Stichwörter der Autor:innen

additive manufacturingdimensional stabilityfatigue behaviorfracture resistanceonlay

Autor:innen und Institutionen

  • Department of Prosthodontics, Faculty of Dentistry, Necmettin Erbakan University, Konya, Turkey.
  • Department of Prosthodontics, Faculty of Dentistry, Biruni University, İstanbul, Turkey.
  • Department of Reconstructive Dentistry and Gerodontology, School of Dental Medicine, University of Bern, Bern, Switzerland.
  • Department of Prosthodontics, School of Dentistry and Dental Research Institute, Seoul National University, Seoul, Republic of Korea.
  • Department of Restorative, Preventive and Pediatric Dentistry, School of Dental Medicine, University of Bern, Bern, Switzerland.
  • Division of Restorative and Prosthetic Dentistry, The Ohio State University, Columbus, Ohio, USA.

ORCID-Profile: Burak Yilmaz

Förderung

  • Buser Implant Foundation Junior Investigator

Zitieren

APA

Güven, M. E., Donmez, M. B., Tezcan, A. N., Yoon, H. I., Yilmaz, B., & Çakmak, G. (2024). Performance and durability of additively and subtractively manufactured resin‐based onlay restorations after thermomechanical aging. Journal of Prosthodontics. https://doi.org/10.1111/jopr.14005

Vancouver

Güven ME, Donmez MB, Tezcan AN, Yoon HI, Yilmaz B, Çakmak G. Performance and durability of additively and subtractively manufactured resin‐based onlay restorations after thermomechanical aging. Journal of Prosthodontics. 2024. doi:10.1111/jopr.14005

BibTeX
@article{Gven2024,
  author = {Güven, Mehmet Esad and Donmez, Mustafa Borga and Tezcan, Ayyüce Nur and Yoon, Hyung-In and Yilmaz, Burak and Çakmak, Gülce},
  title = {Performance and durability of additively and subtractively manufactured resin‐based onlay restorations after thermomechanical aging},
  journal = {Journal of Prosthodontics},
  year = {2024},
  doi = {10.1111/jopr.14005}
}