Mechanical performance and failure analysis of additively manufactured PLA–carbon fibre, PLA–glass fibre, ABS–carbon fibre, and ABS–glass fibre composites
International Polymer Processing · 18.11.2026
DOI: 10.1515/ipp-2026-0093 ↗Kurz gefasst
Fachartikel in der Zeitschrift International Polymer Processing, online erschienen am 18.11.2026. Verfasst von Narayanasamy Pandiarajan und 7 weiteren Autor:innen. Die Arbeit nennt 42 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Universitas Brawijaya.
Abstract (Originalsprache)
The present study investigated the influence of carbon fibre (CF) and glass fibre (GF) reinforcement on the tensile, flexural, and impact properties of FDM-fabricated PLA- and ABS-based composites. Six material systems, namely PLA, CF + PLA, GF + PLA, ABS, CF + ABS, and GF + ABS, were fabricated using a 1.75 mm filament and an FDM process with 100 % infill density, 0 mm air gap, flat (0°) build orientation, and 45° raster angle. Tensile, flexural, and impact tests were conducted according to ASTM D638, ASTM D790, and ASTM D256 standards, respectively. The mechanical performance of the FDM-printed components was significantly impacted by the polymer matrix type, reinforcement type, fibre-matrix interaction, and printing parameters. The fracture surfaces of the fibre-reinforced specimens were further examined using scanning electron microscopy (SEM). Among all the investigated materials, the GF + PLA composites exhibited the highest tensile strength (62.3 MPa), flexural strength (24.6 MPa), and impact strength (88.1 kJ/m 2 ). In addition, the CF + PLA composites showed substantial improvements compared with neat PLA, with tensile, flexural, and impact strengths of 44.8 MPa, 11.2 MPa, and 27.93 kJ/m 2 , respectively. For the ABS, CF + ABS and GF + ABS composites improved tensile strength compared with neat ABS, while the CF + ABS showed better flexural and impact performance than neat ABS. The SEM analysis revealed matrix cracking, fibre pull-out, fibre fracture, matrix deformation, crack deflection, and localized fibre–matrix separation, confirming the involvement of fibre-related load-transfer and fracture mechanisms. Overall, the results demonstrated that the GF + PLA composites provided the most favourable combination of the tensile, flexural, and impact performance under the selected FDM processing conditions.
Förderung
- Universitas Brawijaya
Zitieren
APA
Pandiarajan, N., Setyarini, P. H., Rajaram, P., Selvam, B., Shunmugam, M. N., Ayrilmis, N., Karthekeyan, P. B., & Muniyandi, S. (2026). Mechanical performance and failure analysis of additively manufactured PLA–carbon fibre, PLA–glass fibre, ABS–carbon fibre, and ABS–glass fibre composites. International Polymer Processing. https://doi.org/10.1515/ipp-2026-0093
Vancouver
Pandiarajan N, Setyarini PH, Rajaram P, Selvam B, Shunmugam MN, Ayrilmis N, et al. Mechanical performance and failure analysis of additively manufactured PLA–carbon fibre, PLA–glass fibre, ABS–carbon fibre, and ABS–glass fibre composites. International Polymer Processing. 2026. doi:10.1515/ipp-2026-0093
BibTeX
@article{Pandiarajan2026,
author = {Pandiarajan, Narayanasamy and Setyarini, Putu Hadi and Rajaram, Prithivirajan and Selvam, Baskaran and Shunmugam, Muthu Natarajan and Ayrilmis, Nadir and Karthekeyan, Parrthipan Balasubramaniyan and Muniyandi, Selvakumar},
title = {Mechanical performance and failure analysis of additively manufactured PLA–carbon fibre, PLA–glass fibre, ABS–carbon fibre, and ABS–glass fibre composites},
journal = {International Polymer Processing},
year = {2026},
doi = {10.1515/ipp-2026-0093}
}
EUVIMED