Influence of Different Build Directions on the Fracture Load and Surface Roughness of Additively Manufactured Three-unit Provisional Restoration and Comparison with Conventional Methods of Provisional Fabrication
The International Journal of Prosthodontics · 2024
DOI: 10.11607/ijp.8813 ↗Kurz gefasst
Vergleichsstudie in der Zeitschrift The International Journal of Prosthodontics, 2024. Verfasst von Shubhi Sahni und 3 weiteren Autor:innen. Hauptthemen laut MEDLINE: Dental Restoration, Temporary. Die Arbeit wurde bisher 1-mal zitiert (Crossref).
Abstract (Originalsprache)
PURPOSE: To compare the influence of 0-, 45-, and 90-degree build directions on the fracture load and surface roughness of additively manufactured three-unit fixed provisional restorations and to compare the additively manufactured provisionals to provisionals fabricated using conventional methods. MATERIALS AND METHODS: Mandibular typodont right second molars and premolars were prepared for a missing mandibular first molar to receive a three-unit fixed partial denture. For six groups of 10 samples each, three-unit provisionals were fabricated using additive manufacturing at 0, 45, and 90 degrees; heat polymerized PMMA; autopolymerizing resin; and bis-acryl composites resins-and tested for fracture load and surface roughness. One-way ANOVA and Tukey tests were used to analyze the data. RESULTS: For fracture load, the lowest mean value was for autopolymerizing bis-acryl resin (464.9 N), and the highest value was for additive manufacturing at 0 degrees (596 N). Surface roughness values were lowest for heat-polymerized PMMA (0.132 µm), and the highest value was for autopolymerizing PMMA (0.836 µm). Significant differences were found between the three build directions for fracture load and surface roughness (P = .001); in all pairwise comparisons except between 0 and 90 degrees (P = .502) for fracture load; and between all three build directions for surface roughness (P = .01). Compared to other provisional materials, a significant difference (P = .001) was observed between all groups. CONCLUSIONS: Build direction affected the mechanical properties of additively manufactured three-unit provisionals, with provisionals printed at 0 degrees showing the highest fracture load and lowest surface roughness. Compared to other provisional materials, additively manufactured three-unit provisionals printed at 0 degrees also showed the highest fracture load, with surface roughness similar to heat-polymerized provisionals.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Substanzen
Zitieren
APA
Sahni, S., Kaurani, P., Bhambhu, S., & Yadav, A. (2024). Influence of Different Build Directions on the Fracture Load and Surface Roughness of Additively Manufactured Three-unit Provisional Restoration and Comparison with Conventional Methods of Provisional Fabrication. The International Journal of Prosthodontics. https://doi.org/10.11607/ijp.8813
Vancouver
Sahni S, Kaurani P, Bhambhu S, Yadav A. Influence of Different Build Directions on the Fracture Load and Surface Roughness of Additively Manufactured Three-unit Provisional Restoration and Comparison with Conventional Methods of Provisional Fabrication. The International Journal of Prosthodontics. 2024. doi:10.11607/ijp.8813
BibTeX
@article{Sahni2024,
author = {Sahni, Shubhi and Kaurani, Pragati and Bhambhu, Shweta and Yadav, Anuja},
title = {Influence of Different Build Directions on the Fracture Load and Surface Roughness of Additively Manufactured Three-unit Provisional Restoration and Comparison with Conventional Methods of Provisional Fabrication},
journal = {The International Journal of Prosthodontics},
year = {2024},
doi = {10.11607/ijp.8813}
}
EUVIMED