Fachartikel in der Zeitschrift The International Journal of Prosthodontics, 2023. Verfasst von Abdulaziz Samran und 4 weiteren Autor:innen. Hauptthemen laut MEDLINE: Post and Core Technique, Tooth, Nonvital, Tooth Fractures. Die Arbeit wurde bisher 11-mal zitiert (Crossref).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

PURPOSE: To evaluate the effects of post length, post material, and substance loss on the fracture resistance of endodontically treated mandibular premolars. MATERIALS AND METHODS: A total of 96 extracted human mandibular first premolars were endodontically treated and divided into 12 test groups (n = 8 each) based on the number of residual walls (one/two), post material (glass-fiber/titanium), and post length (5 mm, 7.5 mm, and 10 mm). After luting the posts, specimens received a composite resin core and a crown preparation with a 1.5-mm ferrule. Cast cobalt-chromium crowns were cemented using glass-ionomer cement. After 1,200,000 chewing cycles with a load of 49 N and simultaneous thermocycling (5°C to 55°C), specimens were quasi-statically loaded at 30 degrees to the longitudinal axis of the tooth until fracture. Fracture loads were analyzed using three-way, two-way, and one-way ANOVA (α = .05). Fracture modes were examined under a stereomicroscope (×25 magnification) and recorded. RESULTS: The mean ± SD fracture loads ranged from 642 ± 190 N (one wall, glass fiber, 5 mm) to 1,170 ± 130 N (two walls, titanium, 7.5 mm). The mean fracture load of titanium posts was significantly higher than that of glass-fiber posts (P < .001), and the 7.5-mm post length exhibited significantly higher fracture loads than groups with 5-mm and 10-mm post length (P = .008). CONCLUSIONS: Teeth restored with titanium posts revealed considerably higher fracture resistance than teeth restored with glass-fiber posts, especially if 7.5-mm-length posts were used.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

Post and Core TechniqueTooth, NonvitalTooth FracturesHumansTitaniumCrownsComposite ResinsDental Stress AnalysisDental Restoration Failure

Substanzen

TitaniumComposite Resins

Zitieren

APA

Samran, A., Mourshed, B., Ahmed, M. A., Al-Akhali, M., & Kern, M. (2023). Influence of Post Length, Post Material, and Substance Loss on the Fracture Resistance of Endodontically Treated Teeth: A Laboratory Study. The International Journal of Prosthodontics. https://doi.org/10.11607/ijp.7468

Vancouver

Samran A, Mourshed B, Ahmed MA, Al-Akhali M, Kern M. Influence of Post Length, Post Material, and Substance Loss on the Fracture Resistance of Endodontically Treated Teeth: A Laboratory Study. The International Journal of Prosthodontics. 2023. doi:10.11607/ijp.7468

BibTeX
@article{Samran2023,
  author = {Samran, Abdulaziz and Mourshed, Bilal and Ahmed, Mohammed A and Al-Akhali, Majed and Kern, Matthias},
  title = {Influence of Post Length, Post Material, and Substance Loss on the Fracture Resistance of Endodontically Treated Teeth: A Laboratory Study},
  journal = {The International Journal of Prosthodontics},
  year = {2023},
  doi = {10.11607/ijp.7468}
}
Kostenlos starten →