Influence of post material and ferrule thickness on the fracture resistance of endodontically treated premolars: A laboratory study
The Journal of Prosthetic Dentistry · 2025
DOI: 10.1016/j.prosdent.2024.01.022 ↗Kurz gefasst
Fachartikel in der Zeitschrift The Journal of Prosthetic Dentistry, 2025. Verfasst von Abdulaziz Samran und 5 weiteren Autor:innen. Beteiligte Einrichtung: Visiting Associate Professor, Department of Prosthodontics, Propaedeutics and Dental Materials, School of Dentistry, Christian-Albrechts University, …. Hauptthemen laut MEDLINE: Tooth Fractures, Bicuspid, Post and Core Technique, Tooth, Nonvital. Die Arbeit wurde bisher 8-mal zitiert (Crossref) und nennt 56 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
STATEMENT OF PROBLEM: The influence of the ferrule thickness and post materials on the fracture resistance of endodontically treated teeth remains unclear. PURPOSE: The purpose of this laboratory study was to evaluate the influence of post material and ferrule thickness on the fracture resistance of endodontically treated mandibular premolars. MATERIAL AND METHODS: Sixty-four extracted and endodontically treated mandibular first premolars were used and divided into 4 test groups (n=16) depending on the ferrule thickness: F-0: without a ferrule, F-0.5: with a 0.5-mm ferrule thickness, F-1: with a 1-mm ferrule thickness, and F-1.5: with a 1.5-mm ferrule thickness. In groups with ferrules, the height ranged from 2 mm buccally/lingually to 1 mm proximally. Teeth in subgroups (n=8) were restored with either prefabricated glass fiber (FF) or titanium posts (FT) (ISO size 70 and length of 7.5 mm) and then adhesively restored with composite resin foundation materials. After foundation procedures, each specimen was restored with a cobalt chromium crown which was cemented with glass ionomer cement. All specimens were subjected to dynamic loading in a masticatory simulator for 1 200 000 loading cycles with a nominal load of 5 Kg at 1.2 Hz and simultaneous thermocycling (5 to 55 °C). Specimens were then quasistatically loaded at 30 degrees in a universal testing machine until fracture. Fracture loads were analyzed by using 2-way ANOVA followed by the Tukey honestly significant difference test (α=.05). RESULTS: Fracture loads ranged from 610 ±45 N (no ferrule - glass fiber post) to 1216 ±169 N (1.5 mm ferrule thickness - glass fiber post). A statistically significant increase in fracture resistance was observed with increasing ferrule thickness (P
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Substanzen
Autor:innen und Institutionen
- Visiting Associate Professor, Department of Prosthodontics, Propaedeutics and Dental Materials, School of Dentistry, Christian-Albrechts University, Kiel, Germany; Associate Professor, Department of Restorative and Pros…
- Visiting Assistant Professor, Department of Prosthodontics, Propaedeutics and Dental Materials, School of Dentistry, Christian-Albrechts University, Kiel, Germany; and Lecturer, Faculty of Dentistry, October University…
- Assistant Professor, Department of Prosthodontics, Propaedeutics and Dental Materials, School of Dentistry, Christian-Albrechts University, Kiel, Germany.
- Visiting Assistant Professor, Department of Prosthodontics, Propaedeutics and Dental Materials, Dental School, Christian-Albrechts University, Kiel, Germany; and Assistant Professor, Department of Prosthodontics, Colleg…
- Research Associate, Department of Prosthodontics, Propaedeutics and Dental Materials, School of Dentistry, Christian-Albrechts University, Kiel, Germany.
- Professor and Chairman, Department of Prosthodontics, Propaedeutics and Dental Materials, School of Dentistry, Christian-Albrechts University, Kiel, Germany.
Zitieren
APA
Samran, A., Hashem, A. W., Ali, S., Al-Akhali, M., Wille, S., & Kern, M. (2025). Influence of post material and ferrule thickness on the fracture resistance of endodontically treated premolars: A laboratory study. The Journal of Prosthetic Dentistry. https://doi.org/10.1016/j.prosdent.2024.01.022
Vancouver
Samran A, Hashem AW, Ali S, Al-Akhali M, Wille S, Kern M. Influence of post material and ferrule thickness on the fracture resistance of endodontically treated premolars: A laboratory study. The Journal of Prosthetic Dentistry. 2025. doi:10.1016/j.prosdent.2024.01.022
BibTeX
@article{Samran2025,
author = {Samran, Abdulaziz and Hashem, Ahmed Wagdy and Ali, Shurouk and Al-Akhali, Majed and Wille, Sebastian and Kern, Matthias},
title = {Influence of post material and ferrule thickness on the fracture resistance of endodontically treated premolars: A laboratory study},
journal = {The Journal of Prosthetic Dentistry},
year = {2025},
doi = {10.1016/j.prosdent.2024.01.022}
}
EUVIMED