Fracture strength of anterior cantilever resin‐bonded fixed partial dentures fabricated from high translucency zirconia with different intaglio surface treatments
Journal of Prosthodontics · 2024
DOI: 10.1111/jopr.13694 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Prosthodontics, 2024. Verfasst von Ahed Al-Wahadni und 4 weiteren Autor:innen. Beteiligte Einrichtung: Faculty of Dentistry, Jordan University of Science and Technology, Irbid, Jordan. Hauptthemen laut MEDLINE: Denture, Partial, Fixed, Resin-Bonded, Dental Bonding, Methacrylates. Die Arbeit wurde bisher 6-mal zitiert (Crossref) und nennt 19 Literaturangaben. Gefördert von: Deanship of Scientific Research at Jordan University of Science and Technology.
Abstract (Originalsprache)
Purpose
To compare the fracture resistance and failure modes of anterior cantilever resin‐bonded fixed partial dentures (RBFPDs) fabricated from high translucency zirconia with different intaglio surface treatments. Materials and methods Sound‐extracted canines ( N = 50) were randomly divided into five groups ( n = 10) to be restored with high translucency zirconia RBFBDs of different intaglio surface treatments. The RBFPD was designed using exocad software and fabricated using a CAM milling machine. The RBFPDs were treated differently: abrasion with 50 µm alumina particles (Group 1); abrasion with 30 µm silica‐coated alumina particles (Group 2); abrasion with silica‐coated alumina particles (30 µm) and silane application (Group 3); abrasion with silica‐coated alumina particles (30 µm) and 10‐methacryloyloxydecyl dihydrogen phosphate (10‐MDP) primer application (Group 4); abrasion with silica‐coated alumina particles (30 µm) and silane, and 10‐MDP primer application. All RBFPDs were cemented using dual‐cured resin cement. The RBFPDs underwent 6000 thermal cycles with distilled water at 5/55°C for 2 min per cycle and then mechanical cyclic loading with 1200,000 cycles of 50 N at a 1.7 Hz frequency at an angle of 135° to the abutment's long axis. Then, RBFPDs were loaded to fracture using a universal testing machine at 1 mm/min. Maximum fracture forces and failure modes were recorded. Fractured specimens and uncemented specimens were examined using a scanning electron microscope. Data was analyzed using ANOVA and Games–Howell post hoc tests at p < 0.05.
Results
Mean fracture load results showed a statistically significant difference between the research groups ( p < 0.0001) and it ranged from 69.78 to 584 N. Group 4 exhibited the highest fracture load mean ( p < 0.0001) which was significantly different from all other groups. Group 2 recorded a significantly higher fracture load mean than Group 3 ( p = 0.029). Three modes of failure were observed: prosthesis debonding, prosthesis fracture, and abutment fracture.
Conclusions
Abrasion of zirconia surface with 30 µm silica‐coated alumina particles and application of 10‐MDP primer yielded the highest mean fracture loads of monolithic high translucency zirconia RBFPD. The mode of fracture of the RBFPDs was influenced by the type of surface treatments.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Faculty of Dentistry, Jordan University of Science and Technology, Irbid, Jordan.
- Consultant Clinical Scientist, London, UK.
- Faculty of Applied Medical Sciences, Luminus Technical University College, Amman, Jordan.
- Faculty of Applied Medical Sciences, Jordan University of Science and Technology, Irbid, Jordan.
ORCID-Profile: Ahed Al-Wahadni, Muhanad M Hatamleh
Förderung
- Deanship of Scientific Research at Jordan University of Science and Technology
Zitieren
APA
Al-Wahadni, A., Dkmak, M. S. F., Almohammed, S., Hatamleh, M. M., & Tabanjah, A. (2024). Fracture strength of anterior cantilever resin‐bonded fixed partial dentures fabricated from high translucency zirconia with different intaglio surface treatments. Journal of Prosthodontics. https://doi.org/10.1111/jopr.13694
Vancouver
Al-Wahadni A, Dkmak MSF, Almohammed S, Hatamleh MM, Tabanjah A. Fracture strength of anterior cantilever resin‐bonded fixed partial dentures fabricated from high translucency zirconia with different intaglio surface treatments. Journal of Prosthodontics. 2024. doi:10.1111/jopr.13694
BibTeX
@article{AlWahadni2024,
author = {Al-Wahadni, Ahed and Dkmak, Mhd Salim Fissal and Almohammed, Saleh and Hatamleh, Muhanad M and Tabanjah, Abedelmalek},
title = {Fracture strength of anterior cantilever resin‐bonded fixed partial dentures fabricated from high translucency zirconia with different intaglio surface treatments},
journal = {Journal of Prosthodontics},
year = {2024},
doi = {10.1111/jopr.13694}
}
EUVIMED