EUVIMEDTutustu EUVIMEDiin
Open access · CC BY 4.0

Effect of Glazing Dwell Time and Cooling Duration on Flexural Strength and Surface Microhardness of 3 mol% Yttria‐Stabilized Tetragonal Zirconia: An In Vitro Study

Shubha Sarmalkar iD, Aradhana Nagarsekar iD, Meena A Aras iD, Umesh Y Pai iD, Ridhima Gaunkar iD, Prajakta R Volvaikar iD

Journal of Esthetic and Restorative Dentistry · 2026

DOI: 10.1111/jerd.70232 ↗

At a glance

Journal article in Journal of Esthetic and Restorative Dentistry, 2026. Written by Shubha Sarmalkar and 5 co-authors. Institution: Department of Prosthodontics, Goa Dental College and Hospital, Bambolim, India. Major MEDLINE topics: Zirconium, Yttrium, Dental Materials. 10 references. The full text is freely available (open access, CC BY 4.0).

TiivistelmäSubjectsBibliografiset tiedotCiteRelated studies

Abstract (original language)

Objective

To evaluate the effect of glazing dwell time and cooling duration on the flexural strength and surface microhardness of high‐translucency 3 mol% yttria‐stabilized tetragonal zirconia polycrystal (3Y‐TZP). Materials and Methods Total of 108 rectangular zirconia specimens (20 × 4 × 2 mm) were fabricated from preshaded monolithic blocks and sintered at 1530°C. Specimens were divided into nine groups ( n = 12). The control group (NG) remained unglazed. Experimental groups underwent conventional firing (CF;1‐min dwell) or extended firing (EF; 3‐min dwell) at 850°C, each combined with four cooling durations (4,7,9, or 12 min) between 850°C and 600°C. Flexural strength was evaluated using a four‐point bending test (ISO 6872:2015) with Weibull analysis, while surface microhardness was measured using the Vickers method (50 g, 10 s). Data were analyzed using two‐way ANOVA and Tukey's HSD test ( α = 0.05).

Results

Significant differences were observed in flexural strength and microhardness ( p < 0.001). The unglazed group showed the highest strength (698 ± 18 MPa; m = 46). Among glazed groups, EF3 (3‐min dwell/9‐min cooling) exhibited the highest characteristic strength ( σ ₀ = 657 MPa). EF1 (3‐min dwell/4‐min cooling) showed the lowest strength (466 ± 23 MPa), below ISO requirements. Microhardness decreased with longer cooling durations.

Conclusions

Glazing parameters significantly affect 3Y‐TZP properties. Extended firing with controlled slow cooling (9 min) optimizes strength and reliability, while rapid cooling compromises performance.

Subjects

MeSH terms (MEDLINE)

ZirconiumYttriumDental MaterialsFlexural StrengthSurface PropertiesHardnessTime FactorsMaterials TestingIn Vitro Techniques

Author keywords

Weibull analysiscooling protocolesthetic dentistryflexural strengthglazingmonolithic zirconiasurface microhardness

Substances

ZirconiumYttriumyttria stabilized tetragonal zirconiaDental Materialszirconium oxide

Authors and institutions

  • Department of Prosthodontics, Goa Dental College and Hospital, Bambolim, India.
  • Department of Prosthodontics, Manipal College of Dental Sciences Mangalore, Manipal Academy of Higher Education, Manipal, India.
  • Department of Public Health Dentistry, Goa Dental College and Hospital, Bambolim, India.

ORCID profiles: Shubha Sarmalkar, Aradhana Nagarsekar, Meena A Aras, Umesh Y Pai, Ridhima Gaunkar, Prajakta R Volvaikar

Cite

APA

Sarmalkar, S., Nagarsekar, A., Aras, M. A., Pai, U. Y., Gaunkar, R., & Volvaikar, P. R. (2026). Effect of Glazing Dwell Time and Cooling Duration on Flexural Strength and Surface Microhardness of 3 mol% Yttria‐Stabilized Tetragonal Zirconia: An In Vitro Study. Journal of Esthetic and Restorative Dentistry. https://doi.org/10.1111/jerd.70232

Vancouver

Sarmalkar S, Nagarsekar A, Aras MA, Pai UY, Gaunkar R, Volvaikar PR. Effect of Glazing Dwell Time and Cooling Duration on Flexural Strength and Surface Microhardness of 3 mol% Yttria‐Stabilized Tetragonal Zirconia: An In Vitro Study. Journal of Esthetic and Restorative Dentistry. 2026. doi:10.1111/jerd.70232

BibTeX
@article{Sarmalkar2026,
  author = {Sarmalkar, Shubha and Nagarsekar, Aradhana and Aras, Meena A and Pai, Umesh Y and Gaunkar, Ridhima and Volvaikar, Prajakta R},
  title = {Effect of Glazing Dwell Time and Cooling Duration on Flexural Strength and Surface Microhardness of 3 mol% Yttria‐Stabilized Tetragonal Zirconia: An In Vitro Study},
  journal = {Journal of Esthetic and Restorative Dentistry},
  year = {2026},
  doi = {10.1111/jerd.70232}
}
Start for free →