Evaluation of the physical and mechanical properties of 3D-printed resin for orthodontic fixed lingual retainers: An in vitro study
Journal of Dental Sciences · 2025-07 · 20 (3) · 1723-1730
DOI: 10.1016/j.jds.2025.03.034 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Dental Sciences, 2025-07. Verfasst von Pyi Phyo Win und 5 weiteren Autor:innen. Beteiligte Einrichtung: School of Dentistry, College of Oral Medicine, Taipei Medical University, Taipei, Taiwan. Die Arbeit wurde bisher 5-mal zitiert (Crossref) und nennt 40 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0). Gefördert von: National Science and Technology Council.
Abstract (Originalsprache)
Background/Purpose: Fixed lingual retainers (FLRs) often experience structural instability, including poor adaptation, and the untwisting of spiral wires, which can lead to unwanted tooth movement. Digital workflows have enhanced the appliance's accuracy. This study evaluated the water sorption (Wsp), water solubility (Wsl), staining resistance, and flexural performance of three-dimensionally printed resin (3DR) to determine its optimal design for FLRs. Materials and methods: Cylindrical 3DR specimens were immersed in distilled water and artificial saliva for 7, 14, and 30 days. Wsp and Wsl were measured according to ISO 4049 guidelines. Color stability was analyzed after 7 days of immersion in staining solutions using the CIEDE2000 formula. Straight 3DR specimens with various cross-sectional shapes and dimensions underwent a three-point bending test, comparing mechanical properties to multistrand stainless-steel wire (MSW). Statistical analysis was performed using a one-way ANOVA with Tukey's post-hoc test (P < 0.05).
Results
Wsp and Wsl values remained within ISO standards, with no significant changes over time. Specimens exposed to red wine, grape juice, and curry exhibited color changes exceeding the acceptability threshold of 1.77, while other solutions caused minimal discoloration. Hemi-elliptical cross-sections demonstrated significantly greater flexural strength than round designs. Although all 3DR specimens fractured before reaching the 2.0-mm deflection limit, some designs exhibited comparable bending strength to MSW while maintaining sufficient flexibility for physiological tooth movement.
Conclusion
A hemi-elliptical 3DR design (1.0 mm thick and 2.0 mm wide) demonstrated stability in the oral environment, moderate stainability, and mechanical performance comparable to MSW, supporting its feasibility for FLRs.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- School of Dentistry, College of Oral Medicine, Taipei Medical University, Taipei, Taiwan.
- Division of Orthodontics, Department of Dentistry, Taipei Medical University Hospital, Taipei, Taiwan.
- School of Dentistry, Mongolian National University of Medical Sciences, Ulaanbaatar City, Mongolia.
Förderung
- National Science and Technology Council
Zitieren
APA
Win, P. P., Lai, S. Y., De-Shing Chen, D., Sainbayar, B., Peng, T. Y., & Hsin-Chung Cheng, J. (2025). Evaluation of the physical and mechanical properties of 3D-printed resin for orthodontic fixed lingual retainers: An in vitro study. Journal of Dental Sciences, 20(3), 1723-1730. https://doi.org/10.1016/j.jds.2025.03.034
Vancouver
Win PP, Lai SY, De-Shing Chen D, Sainbayar B, Peng TY, Hsin-Chung Cheng J. Evaluation of the physical and mechanical properties of 3D-printed resin for orthodontic fixed lingual retainers: An in vitro study. Journal of Dental Sciences. 2025;20(3):1723-1730. doi:10.1016/j.jds.2025.03.034
BibTeX
@article{Win2025,
author = {Win, Pyi Phyo and Lai, Szu-Yu and De-Shing Chen, Daniel and Sainbayar, Bolormaa and Peng, Tzu-Yu and Hsin-Chung Cheng, Johnson},
title = {Evaluation of the physical and mechanical properties of 3D-printed resin for orthodontic fixed lingual retainers: An in vitro study},
journal = {Journal of Dental Sciences},
year = {2025},
volume = {20},
number = {3},
pages = {1723--1730},
doi = {10.1016/j.jds.2025.03.034}
}
EUVIMED