A Novel 3‐Dimensional Printed Nanoceramic Hybrid Resin Fixed Lingual Retainer: Characterization and Mechanical Tests
International Journal of Dentistry · 2024-01 · 2024 (1)
DOI: 10.1155/2024/3540846 ↗Kurz gefasst
Fachartikel in der Zeitschrift International Journal of Dentistry, online erschienen am 14.10.2024. Verfasst von Noor Salam Alnuaimy und 1 weiteren Autor:innen. Beteiligte Einrichtung: Department of Orthodontics, College of Dentistry, University of Baghdad, Baghdad, Iraq. Die Arbeit wurde bisher 3-mal zitiert (Crossref) und nennt 63 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
Introduction
An innovative retention protocol was developed to create a new 3D‐printed fixed retainer employing SprintRay OnX nanoceramic hybrid resin. The feasibility and usability of the retainer were subsequently evaluated.
Methods
Identification and characterization of SprintRay OnX was done using Fourier transform infrared spectroscopy (FTIR), scanning electron microscopy with energy dispersive X‐ray (SEM‐EDX), field emission scanning electron microscope (FE‐SEM), X‐ray diffraction (XRD), and flexural strength. Load–deflection and pull‐out tests were conducted on the 3D‐printed straight wires, with three distinct cross‐sectional geometries: round (1 mm), oval (1 mm × 1.5 mm) and semielliptical (1 mm × 1.5 mm). Twisted G&H and coaxial Respond stainless steel multistrand retainers were used for comparison. In the load–deflection test, a three‐point bending test (3PBT) was employed. For the pull‐out test, the retainer wire was inserted into the composite, which was placed in a centrally located hole of an acrylic block; the retainer wire was subjected to a tensile force along its long axis.
Results
Characteristic bands close to those of PMMA were observed in the FTIR spectra. SEM‐EDX and XRD revealed a crystalline material with homogeneously distributed Yb element signals (19.4%). On FE‐SEM micrographs, small clumps were displayed on smooth surfaces. The flexural strength and the flexural modulus were, respectively, 142.48 MPa and 7.842 GPa. All groups of 3D‐printed wires exhibited significantly higher load–deflection levels than the multistrand wires (MSWs). Concerning pull‐out forces, they fell in between twisted G&H (96 N) and coaxial Respond (48.09 N) retainer wires. The 3D‐printed wires fractured cohesively without detachment from the adhesive, suggesting that the chemical bond was adequate for satisfactory wire integration, yet the wire’s strength was compromised. Concerning the cross‐sectional geometry, the load–deflection and the pull‐out forces of 3D‐printed oval and semielliptical wires were significantly higher than that of 3D‐printed round wires, which was attributed to the larger cross‐sections of the wires.
Conclusion
Oval and semielliptical 3D‐printed wires offered favorable features as lingual retainers.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Department of Orthodontics, College of Dentistry, University of Baghdad, Baghdad, Iraq.
ORCID-Profile: Noor Salam Alnuaimy, Akram Faisal Alhuwaizi
Zitieren
APA
Alnuaimy, N. S., & Alhuwaizi, A. F. (2024). A Novel 3‐Dimensional Printed Nanoceramic Hybrid Resin Fixed Lingual Retainer: Characterization and Mechanical Tests. International Journal of Dentistry, 2024(1). https://doi.org/10.1155/2024/3540846
Vancouver
Alnuaimy NS, Alhuwaizi AF. A Novel 3‐Dimensional Printed Nanoceramic Hybrid Resin Fixed Lingual Retainer: Characterization and Mechanical Tests. International Journal of Dentistry. 2024;2024(1). doi:10.1155/2024/3540846
BibTeX
@article{Alnuaimy2024,
author = {Alnuaimy, Noor Salam and Alhuwaizi, Akram Faisal},
title = {A Novel 3‐Dimensional Printed Nanoceramic Hybrid Resin Fixed Lingual Retainer: Characterization and Mechanical Tests},
journal = {International Journal of Dentistry},
year = {2024},
volume = {2024},
number = {1},
doi = {10.1155/2024/3540846}
}
EUVIMED