Repair of monolithic zirconia restorations with different direct resin composites: effect on the fatigue bonding and mechanical performance
Clinical Oral Investigations · 2024
DOI: 10.1007/s00784-024-05542-4 ↗Kurz gefasst
Fachartikel in der Zeitschrift Clinical Oral Investigations, 2024. Verfasst von Pablo Machado Soares und 9 weiteren Autor:innen. Beteiligte Einrichtung: Post-Graduate Program in Oral Sciences, Center for Development of Advanced Materials, Division of Prosthodontics-Biomaterials, Federal University of …. Hauptthemen laut MEDLINE: Dental Bonding, Methacrylates. Die Arbeit wurde bisher 11-mal zitiert (Crossref) und nennt 36 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Brazilian Federal Agency for Coordination of Improvement of Higher Education Personnel - CAPES, Brazilian National Council for Scientific and Technological Development - CNPq, Brazilian Federal Agency for Coordination of Improvement of Higher Education Personnel – CAPES.
Abstract (Originalsprache)
Objective
The study aims to evaluate the shear bond and flexural strength fatigue behavior of yttrium-stabilized zirconia (4YSZ) repaired using different resin composites. Materials and methods Cylindric specimens of 4YSZ were obtained for the bond strength (Ø = 6 mm, 1.5 mm of thickness) and biaxial flexural strength (Ø = 15 mm, 1 mm of thickness) fatigue tests and divided into 3 groups according to the repair resin composite: EVO (nanohybrid), BULK (bulk-fill), and FLOW (flowable). The zirconia surface was air-abraded with alumina particles, a 10-methacryloyloxydecyl dihydrogen phosphate (10-MDP) primer was applied, and the resin composite was build-up over the zirconia. Fatigue shear bond strength and flexural fatigue strength tests were performed ( n = 15). One-way ANOVA and Tukey post hoc tests were carried out for both outcomes, besides scanning electron microscopy and finite element analysis.
Results
The repair material affected the fatigue shear bond strength of zirconia ceramic. The BULK group (18.9 MPa) depicted higher bond strength values than FLOW (14.8 MPa) ( p = 0.04), while EVO (18.0 MPa) showed similar results to both groups. No effect was observed for the mechanical behavior ( p = 0.53). The stress distribution was similar for all groups.
Conclusion
The repair of yttrium-stabilized zirconia (4YSZ) ceramics with bulk-fill resin composites was the best option for high fatigue bond strength. However, the fatigue mechanical performance was similar regardless of the applied repair material. Clinical relevance The repair of yttrium-stabilized zirconia (4YSZ) monolithic restorations may be performed with nanohybrid and bulk-fill resin composites in order to promote longevity in the treatment.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Post-Graduate Program in Oral Sciences, Center for Development of Advanced Materials, Division of Prosthodontics-Biomaterials, Federal University of Santa Maria (UFSM), Santa Maria, Brazil.
- Department of Dental Materials Science, Academic Centre for Dentistry Amsterdam (ACTA), Universiteit Van Amsterdam and Vrije Universiteit, Amsterdam, North Holland, the Netherlands.
- Department of Reconstructive Oral Care, Academic Centre for Dentistry Amsterdam (ACTA), Universiteit Van Amsterdam and Vrije Universiteit, Amsterdam, North Holland, the Netherlands. j.p.mendes.tribst@acta.nl.
Förderung
- Brazilian Federal Agency for Coordination of Improvement of Higher Education Personnel - CAPES
- Brazilian National Council for Scientific and Technological Development - CNPq
- Brazilian Federal Agency for Coordination of Improvement of Higher Education Personnel – CAPES
- Brazilian National Council for Scientific and Technological Development – CNPq
Zitieren
APA
Soares, P. M., da Rosa, L. S., Pilecco, R. O., Dal Piva, A. M. O., Tribst, J. P. M., Werner, A., Valandro, L. F., Pereira, G. K. R., Kleverlaan, C. J., & Rippe, M. P. (2024). Repair of monolithic zirconia restorations with different direct resin composites: effect on the fatigue bonding and mechanical performance. Clinical Oral Investigations. https://doi.org/10.1007/s00784-024-05542-4
Vancouver
Soares PM, da Rosa LS, Pilecco RO, Dal Piva AMO, Tribst JPM, Werner A, et al. Repair of monolithic zirconia restorations with different direct resin composites: effect on the fatigue bonding and mechanical performance. Clinical Oral Investigations. 2024. doi:10.1007/s00784-024-05542-4
BibTeX
@article{Soares2024,
author = {Soares, Pablo Machado and da Rosa, Lucas Saldanha and Pilecco, Rafaela Oliveira and Dal Piva, Amanda Maria de Oliveira and Tribst, João Paulo Mendes and Werner, Arie and Valandro, Luiz Felipe and Pereira, Gabriel Kalil Rocha and Kleverlaan, Cornelis Johannes and Rippe, Marilia Pivetta},
title = {Repair of monolithic zirconia restorations with different direct resin composites: effect on the fatigue bonding and mechanical performance},
journal = {Clinical Oral Investigations},
year = {2024},
doi = {10.1007/s00784-024-05542-4}
}
EUVIMED