The effect of different surface treatments on the bond strength to zirconia
Journal of Prosthodontics · 2025
DOI: 10.1111/jopr.14068 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Prosthodontics, 2025. Verfasst von Kushaldeep Fnu und 7 weiteren Autor:innen. Beteiligte Einrichtung: Department of Restorative Dentistry, Temple University Kornberg School of Dentistry, Pennsylvania, USA. Hauptthemen laut MEDLINE: Zirconium, Dental Bonding, Dental Etching, Dental Materials. Die Arbeit nennt 37 Literaturangaben.
Abstract (Originalsprache)
Purpose
To evaluate the effect of various surface treatment methods on zirconia as it affects the bond strength to its substrate. Materials and Methods Sintered zirconium dioxide ceramic disks (KATANA Zirconia STML; n = 20; size 12 × 12 × 3 mm) were divided into five groups: no surface treatment (Group C), air‐particle abraded with 50 µm aluminum oxide (Group AA), air‐particle abraded with glass beads (Group GB), Zircos E etching solution for 2 h (Group ZE), and 48% hydrofluoric acid solution heated at 25°C for 30 min (Group HE). Cylindrical composite resin specimens (2.1 mm in diameter, 3 mm in height) were bonded to the zirconia samples with resin cement (Panavia V5) under a load of 1000 g and light cured for 80 s. Each group was divided into two subgroups, and shear bond strength (SBS) was tested at a crosshead speed of 1 mm/min after storage in distilled water for 24 h at 37°C or after 10,000 thermocycles. The fractured surfaces of specimens were inspected with a stereo microscope, and failure modes were classified as adhesive, cohesive, or mixed failures. One‐way ANOVA test and paired t ‐test were applied for statistical analysis.
Results
Highest mean SBS values [MPa] were observed for Group AA (14.98 ± 3.19) followed by Group HF (14.8 ± 0.83), Group C (8.32 ± 1.95), Group GB (9.29 ± 0.99), and Group ZE (4.83 ± 0.47). Mean SBS values (MPa) of all the groups decreased significantly after thermal cycling and were for 5.45 ± 0.8 (Group C), 13.47 ± 2.33 (Group AA), 8.56 ± 1.35 (Group GB), 4.16 ± 0.63 (Group ZE), and 13.15 ± 1.27 (Group HF).
Conclusions
Air‐particle abrasion with alumina and heated 48% hydrofluoric acid provide higher bond strengths than the other surface treatments tested.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Department of Restorative Dentistry, Temple University Kornberg School of Dentistry, Pennsylvania, USA.
- Division of Restorative Dentistry, Preventive and Restorative Sciences Department, School of Dental Medicine, University of Pennsylvania, Pennsylvania, USA.
- Department of Prosthodontics, D.A.V. (C) Dental College, Yamana Nagar, Haryana, India.
ORCID-Profile: Kushaldeep Fnu
Zitieren
APA
Fnu, K., Musharbash, L., Ozer, F., Mante, F., Conejo, J., Upadhyaya, V., Anadioti, E., & Blatz, M. B. (2025). The effect of different surface treatments on the bond strength to zirconia. Journal of Prosthodontics. https://doi.org/10.1111/jopr.14068
Vancouver
Fnu K, Musharbash L, Ozer F, Mante F, Conejo J, Upadhyaya V, et al. The effect of different surface treatments on the bond strength to zirconia. Journal of Prosthodontics. 2025. doi:10.1111/jopr.14068
BibTeX
@article{Fnu2025,
author = {Fnu, Kushaldeep and Musharbash, Leen and Ozer, Fusun and Mante, Francis and Conejo, Julian and Upadhyaya, Viram and Anadioti, Eva and Blatz, Markus B},
title = {The effect of different surface treatments on the bond strength to zirconia},
journal = {Journal of Prosthodontics},
year = {2025},
doi = {10.1111/jopr.14068}
}
EUVIMED