Fachartikel in der Zeitschrift Rafidain Oral and Dental Research Journal, online erschienen am 18.07.2026. Verfasst von Diana Qasim sabih und 5 weiteren Autor:innen. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-SA 4.0).
Abstract (Originalsprache)
Background: implant-supported crowns are widely used for the replacement of missing teeth. Recent advances in digital dentistry have introduced CAD/CAM and 3D-printing technologies, providing a variety of restorative materials with different mechanical properties. However, evidence regarding their fracture behavior and failure patterns remains limited.
Objective
To compare the fracture patterns of CAD/CAM nano-hybrid ceramic, 3D printed resin matrix ceramic, and zirconia implant supported crowns Material and method: vericom Mazic® Duro (CAD/CAM Nano Hybrid Ceramic) and saremco Print Crowntec (3D printable resins-based) were used as resin matrix ceramic and IPS e.max. ZirCAD ivoclar (zirconia) was utilized to fabricate lower first molar screw-retained, implant-supported crowns. following fabrication, the crowns were glued onto stock abutments-previously secured to analogs embedded in acrylic resin -using Rely X U200 self-adhesive resin cement (3M ESPE, Germany) . At last , all specimens were subjected to a fracture resistance test. Chi-square was applied to assess the fracture patterns.
Results
Statistical evaluation using the chi-square test revealed no significant relationship between fracture mode and methods (p-value =0.109) .The failure mode in Group A and Group B showed that all specimens failed due to crown fracture, with 83.3% exhibiting mode 1 (Crown fracture) and the remaining 16.7% experiencing mode 2 (Crown fracture + total debonding). In Group C, the failure modes were evenly distributed, with 50% classified as mode 1 and the remaining 50% as mode 2.
Conclusion
The different materials do not impact the mechanism of fracture of an implant-supported crown. The higher incidence of debonding in zirconia crowns may be related to the absence of silica on the zirconia surface
Zitieren
APA
sabih, D. Q., Jasim, H. H., Mahdi, N. A., Bourgi, R., Al-Bazaza, F. A. M., & Naji, A. N. (2026). Comparative Evaluation of Fracture Patterns of CAD/CAM, 3D-Printed Resin Matrix Ceramic, and Zirconia Implant-Supported Crowns. Rafidain Oral and Dental Research Journal, 01-08. https://doi.org/10.69049/rodrj.v1.i1.a4
Vancouver
sabih DQ, Jasim HH, Mahdi NA, Bourgi R, Al-Bazaza FAM, Naji AN. Comparative Evaluation of Fracture Patterns of CAD/CAM, 3D-Printed Resin Matrix Ceramic, and Zirconia Implant-Supported Crowns. Rafidain Oral and Dental Research Journal. 2026:01-08. doi:10.69049/rodrj.v1.i1.a4
BibTeX
@article{sabih2026,
author = {sabih, Diana Qasim and Jasim, Haider Hasan and Mahdi, Nada Ali and Bourgi, Rim and Al-Bazaza, Farah Abdul-Razzaq Mahmood and Naji, Aya Nashwan},
title = {Comparative Evaluation of Fracture Patterns of CAD/CAM, 3D-Printed Resin Matrix Ceramic, and Zirconia Implant-Supported Crowns},
journal = {Rafidain Oral and Dental Research Journal},
year = {2026},
pages = {01--08},
doi = {10.69049/rodrj.v1.i1.a4}
}
EUVIMED