Printing Orientation and Layer Thickness of Nitrogen Post-Cured LCD 3D-Printed Dental Resins

Al-Hakam Jalil Ibrahim Al-Azzawi, Hussein Ahmed Al-Khafaji, Safa Muneer Abdulsattar, Ali F. AlQrimli

Dentistry 3000 · 30.06.2026 · 14 (1)

DOI: 10.5195/d3000.2026.1470 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Dentistry 3000, online erschienen am 30.06.2026. Verfasst von Al-Hakam Jalil Ibrahim Al-Azzawi und 3 weiteren Autor:innen. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study investigated the impact of two printing orientations (45° and 90°) and two-layer thicknesses (50 µm and 100 µm) on the compressive, tensile, and flexural strengths of a 3D-printed dental resin post-cured in a controlled nitrogen atmosphere. A total of 120 specimens were virtually designed according to ISO standards and then fabricated utilizing an LCD-based 3D printer (SOL, Ackuretta). The specimens were divided into four groups (n = 30/group). All specimens underwent post-curing in a nitrogen (N₂) atmosphere and were tested using a universal testing machine. Data analysis was performed using two-way ANOVA and Tukey's HSD test. Group 2 (45° orientation, 50 µm layer thickness) exhibited significantly higher compressive strength (138.2 ± 11.9 MPa) compared to all other groups (p < 0.001). Tensile strength showed no statistically significant differences among the tested groups (p > 0.05). Specimens printed at a 90° orientation demonstrated significantly higher flexural strength compared to the 45° groups (p < 0.001), with printing orientation exhibiting a greater influence than layer thickness. The compressive and flexural strengths of the tested resin are highly affected by the changes in printing parameters, whereas the tensile strength remained statistically unaffected among the groups. The ideal setting for restorations bearing compressive loads is a 45° orientation with a 50 µm layer thickness, whereas a 90° orientation is highly recommended for long-span restorations subject to flexural loads.

Zitieren

APA

Al-Azzawi, A. J. I., Al-Khafaji, H. A., Abdulsattar, S. M., & AlQrimli, A. F. (2026). Printing Orientation and Layer Thickness of Nitrogen Post-Cured LCD 3D-Printed Dental Resins. Dentistry 3000, 14(1). https://doi.org/10.5195/d3000.2026.1470

Vancouver

Al-Azzawi AJI, Al-Khafaji HA, Abdulsattar SM, AlQrimli AF. Printing Orientation and Layer Thickness of Nitrogen Post-Cured LCD 3D-Printed Dental Resins. Dentistry 3000. 2026;14(1). doi:10.5195/d3000.2026.1470

BibTeX
@article{AlAzzawi2026,
  author = {Al-Azzawi, Al-Hakam Jalil Ibrahim and Al-Khafaji, Hussein Ahmed and Abdulsattar, Safa Muneer and AlQrimli, Ali F.},
  title = {Printing Orientation and Layer Thickness of Nitrogen Post-Cured LCD 3D-Printed Dental Resins},
  journal = {Dentistry 3000},
  year = {2026},
  volume = {14},
  number = {1},
  doi = {10.5195/d3000.2026.1470}
}
Kostenlos starten →