The formation of high-quality ohmic contacts on the backside of thinned SiC wafers is critical for vertical power devices to minimize specific on-resistance and enhance energy efficiency. Conventional green laser (532 nm) annealing for Ni-based backside metallization faces challenges such as severe carbon out-diffusion, interfacial voids, and high contact resistivity. This work introduces a Ni/Ti composite metallization scheme combined with 355 nm ultraviolet laser annealing (UV-LA) to address these limitations. By replacing the Ni single-layer with a Ni/Ti stack layer, the reflectivity at 355 nm UV laser annealing is reduced, enabling efficient energy absorption and localized alloying. Ti acts as a diffusion barrier, suppressing Kirkendall void formation and immobilizing carbon through in-situ TiC formation, as confirmed by XRD analyses. Additionally, UV-LA at 4.2 J/cm² with Ni/Ti composite metallization optimizes reaction kinetics, achieving a 69% reduction in void density and a 65% improvement in alloy layer flatness compared to Ni alloy layer. The results validate Ni/Ti-UV-LA as a scalable solution for high-reliability SiC backside metallization, paving the way for next-generation power devices.
Zitieren
APA
Yang, S. L., Luo, Y. H., Yao, Y., Cheng, Y. H., & Zhu, Q. W. (2026). Low-Defect Ni/Ti Composite Backside Ohmic Contact for Thinned 4H-SiC Devices Formed by 355 Nm UV Laser Annealing. Engineering Innovations, 18, 1-5. https://doi.org/10.4028/p-5ptqpk
Vancouver
Yang SL, Luo YH, Yao Y, Cheng YH, Zhu QW. Low-Defect Ni/Ti Composite Backside Ohmic Contact for Thinned 4H-SiC Devices Formed by 355 Nm UV Laser Annealing. Engineering Innovations. 2026;18:1-5. doi:10.4028/p-5ptqpk
BibTeX
@article{Yang2026,
author = {Yang, Song Lin and Luo, Ye Hui and Yao, Yao and Cheng, Yin Hua and Zhu, Qi Wei},
title = {Low-Defect Ni/Ti Composite Backside Ohmic Contact for Thinned 4H-SiC Devices Formed by 355 Nm UV Laser Annealing},
journal = {Engineering Innovations},
year = {2026},
volume = {18},
pages = {1--5},
doi = {10.4028/p-5ptqpk}
}
EUVIMED