Ti/TaSi2/Pt Metallization on n-Type 4H-SiC: Effects of the Thickness Ratio and Annealing on Ohmic Contact Stability at 600 °C

Yongwei Li, Shilin Liu, Zhiqiang Li, Jing Lu, Cheng Lei, Jiangang Yu, Pinggang Jia, Zhicheng Zhao, Ting Liang

Crystals · 09.11.2026 · 16 (11) · 711

DOI: 10.3390/cryst16110711 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Crystals, online erschienen am 09.11.2026. Verfasst von Yongwei Li und 8 weiteren Autor:innen. Die Arbeit nennt 33 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: the National Key Research and Development Program of China, the Open Fund of the State Key Laboratory of Extreme Environment Optoelectronic Dynamic Measurement Technology and Instrument, the Science and Technology Major Program of Shanxi Province.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

To improve the stability of ohmic contacts for SiC sensor chips operating at 600 °C, SiC/Ti/TaSi2/Pt ohmic contact stacks were fabricated on n-type 4H-SiC in this work. The effects of the Ti/TaSi2/Pt thickness ratio and annealing conditions on electrode performance were systematically investigated, and the resulting electrodes were characterized via SEM, XRD and AES. The results show that a lower specific contact resistivity (SCR) (7.16 × 10−5 Ω·cm2) is obtained after the Ti/TaSi2/Pt ratio of 1:3:2 (50/150/100 nm) is rapidly annealed at 1050 °C. The SCR remains 3.05 × 10−4 Ω·cm2 after 20 h of atmospheric aging at 600 °C, and the electrode surface remains flat enough for the subsequent processes. Taken together, the XRD and AES results suggest that the formation of well-crystallized TiC/TaC and Si-enriched titanium silicides lowers the specific contact resistance, and that the thermally stable phases, such as TaC, hinder oxygen ingress, which is consistent with the observed high-temperature stability. In contrast, oxygen penetrates into the contact interface and forms TiO2, an insulating oxide that increases the contact resistance and thereby degrades the contact performance. The results provide a basis for the design of ohmic contacts for high-temperature silicon carbide sensors.

Förderung

  • the National Key Research and Development Program of China
  • the Open Fund of the State Key Laboratory of Extreme Environment Optoelectronic Dynamic Measurement Technology and Instrument
  • the Science and Technology Major Program of Shanxi Province
  • the Key Research and Development Program of Shanxi Province
  • Shanxi Province Major Science and Technology Special Project

Zitieren

APA

Li, Y., Liu, S., Li, Z., Lu, J., Lei, C., Yu, J., Jia, P., Zhao, Z., & Liang, T. (2026). Ti/TaSi2/Pt Metallization on n-Type 4H-SiC: Effects of the Thickness Ratio and Annealing on Ohmic Contact Stability at 600 °C. Crystals, 16(11), 711. https://doi.org/10.3390/cryst16110711

Vancouver

Li Y, Liu S, Li Z, Lu J, Lei C, Yu J, et al. Ti/TaSi2/Pt Metallization on n-Type 4H-SiC: Effects of the Thickness Ratio and Annealing on Ohmic Contact Stability at 600 °C. Crystals. 2026;16(11):711. doi:10.3390/cryst16110711

BibTeX
@article{Li2026,
  author = {Li, Yongwei and Liu, Shilin and Li, Zhiqiang and Lu, Jing and Lei, Cheng and Yu, Jiangang and Jia, Pinggang and Zhao, Zhicheng and Liang, Ting},
  title = {Ti/TaSi2/Pt Metallization on n-Type 4H-SiC: Effects of the Thickness Ratio and Annealing on Ohmic Contact Stability at 600 °C},
  journal = {Crystals},
  year = {2026},
  volume = {16},
  number = {11},
  pages = {711},
  doi = {10.3390/cryst16110711}
}
Kostenlos starten →