Immediate and Delayed Repair Bond Strength of Amalgam -Composite Resin with Various Universal Adhesives and Surface Treatments

Razieh Hoseinifar, Niloofar Shadman, Elaheh Mortazavi Lahijani, Laleh Asadi, Sara Rezaee

Journal of Kerman University of Medical Sciences · 02.05.2026 · 33 · 4097

DOI: 10.34172/jkmu.4097 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Kerman University of Medical Sciences, online erschienen am 02.05.2026. Verfasst von Razieh Hoseinifar und 4 weiteren Autor:innen. Die Arbeit nennt 32 Literaturangaben.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Introduction

Amalgam is a safe and effective option for direct restorations. For amalgam repairs, it is recommended to use composite resin along with an adhesive agent on pretreated amalgam surfaces. This study investigated the shear bond strength (SBS) between composite and both new and aged amalgam, using different universal adhesives on the pretreated alloy surfaces.

Methods

In this experimental in-vitro study, a total of 132 amalgam discs were prepared and divided into two main groups: fresh and aged (6 months water storage + 2000 thermal cycles). The aged amalgam specimens were randomly treated with sandblasting, pumice, or bur. Based on the type of adhesive used, each treated group was further divided into three subgroups: Single Bond Universal, Clearfil Universal Bond, and G-Premio Bond. Fresh amalgam groups were randomly divided into the Single Bond Universal and Clearfil Universal Bond subgroups. All samples were repaired with composite and then subjected to 2000 thermal cycles, followed by SBS assessment using a universal testing machine. One-way and two-way ANOVA, post-hoc Tukey’s, Kruskal-Wallis, Mann-Whitney, and T-tests were used for statistical analysis.

Results

Single Bond Universal + pumice exhibited the highest SBS and Clearfil Universal Bond + bur was associated with the lowest SBS. Among the aged samples, groups prepared with bur had significantly lower SBS values compared to those treated with sandblasting or pumice. The SBS values for the Single Bond Universal groups were significantly greater than those for the Clearfil Universal Bond groups.

Conclusion

Pretreatment with pumice and sandblasting yielded the highest SBS between aged amalgam and composite. Furthermore, Single Bond Universal resulted in the best SBS values.

Zitieren

APA

Hoseinifar, R., Shadman, N., Lahijani, E. M., Asadi, L., & Rezaee, S. (2026). Immediate and Delayed Repair Bond Strength of Amalgam -Composite Resin with Various Universal Adhesives and Surface Treatments. Journal of Kerman University of Medical Sciences, 33, 4097. https://doi.org/10.34172/jkmu.4097

Vancouver

Hoseinifar R, Shadman N, Lahijani EM, Asadi L, Rezaee S. Immediate and Delayed Repair Bond Strength of Amalgam -Composite Resin with Various Universal Adhesives and Surface Treatments. Journal of Kerman University of Medical Sciences. 2026;33:4097. doi:10.34172/jkmu.4097

BibTeX
@article{Hoseinifar2026,
  author = {Hoseinifar, Razieh and Shadman, Niloofar and Lahijani, Elaheh Mortazavi and Asadi, Laleh and Rezaee, Sara},
  title = {Immediate and Delayed Repair Bond Strength of Amalgam -Composite Resin with Various Universal Adhesives and Surface Treatments},
  journal = {Journal of Kerman University of Medical Sciences},
  year = {2026},
  volume = {33},
  pages = {4097},
  doi = {10.34172/jkmu.4097}
}
Kostenlos starten →