The Effect of Different Chemical Surface Treatments on the Bond Strength of Resin-Matrix Ceramic Repaired with Resin Composite

Satit Prabriputaloong, Nantawan Krajangta, Awiruth Klaisiri iD

European Journal of Dentistry · 01.02.2025 · 19 (01) · 165-172

DOI: 10.1055/s-0044-1785531 ↗

Kurz gefasst

Fachartikel in der Zeitschrift European Journal of Dentistry, erschienen am 01.02.2025. Verfasst von Satit Prabriputaloong und 2 weiteren Autor:innen. Beteiligte Einrichtung: Division of Restorative Dentistry, Faculty of Dentistry, Thammasat University, Pathum Thani, Thailand. Die Arbeit wurde bisher 8-mal zitiert (Crossref) und nennt 34 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Thammasat University Research Fund of Thammasat University, Thailand.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Objective

This study investigates the effect of different chemical surface treatment protocols with different functional monomers of universal adhesives on the shear bond strength between resin-matrix ceramic and resin composite. Materials and Methods Eighty resin-matrix ceramics (Shofu block HC) were built and designed into eight groups of ten specimens and surface treated with HC primer (HC) and/or three universal adhesives (single bond universal [SBU], Scotchbond universal plus [SBP], and Tetric N-bond universal [TNU]) assigning follows; group 1, nonsurface treated; group 2, HC; group 3, SBU; group 4, HC + SBU; group 5, SBP; group 6, HC + SBP; group 7, TNU; group 8, HC + TNU. A template was put on the specimen center, and then pushed packable resin composite. Mechanical testing machinery was used to examine the samples' shear bond strength (SBS) values. To examine failure patterns, the debonded specimen surfaces were examined by a stereomicroscope. Statistical Analysis The one-way analysis of variance method was used to evaluate the data, and the Tukey's test was used to determine the significant level (p < 0.05).

Results

The highest SBS was obtained in group 6 (39.25 ± 1.65 MPa). Group 1 (4.15 ± 0.54 MPa) had the lowest SBS. Group 6 exhibited the highest percentage of cohesive failure patterns (70%). High SBS values were frequently correlated with the surface treatment groups and the cohesive failure patterns.

Conclusion

The application of HC primer prior to the universal adhesive is an alternative protocol for enhancing the repair bond strength between resin-matrix ceramic and resin composite interfaces. Moreover, the application of HC primer prior to the SBP is the best strategy for resin-matrix ceramic and resin composite repairs.

Autor:innen und Institutionen

  • Division of Restorative Dentistry, Faculty of Dentistry, Thammasat University, Pathum Thani, Thailand.

ORCID-Profile: Awiruth Klaisiri

Förderung

  • Thammasat University Research Fund of Thammasat University, Thailand

Zitieren

APA

Prabriputaloong, S., Krajangta, N., & Klaisiri, A. (2025). The Effect of Different Chemical Surface Treatments on the Bond Strength of Resin-Matrix Ceramic Repaired with Resin Composite. European Journal of Dentistry, 19(01), 165-172. https://doi.org/10.1055/s-0044-1785531

Vancouver

Prabriputaloong S, Krajangta N, Klaisiri A. The Effect of Different Chemical Surface Treatments on the Bond Strength of Resin-Matrix Ceramic Repaired with Resin Composite. European Journal of Dentistry. 2025;19(01):165-172. doi:10.1055/s-0044-1785531

BibTeX
@article{Prabriputaloong2025,
  author = {Prabriputaloong, Satit and Krajangta, Nantawan and Klaisiri, Awiruth},
  title = {The Effect of Different Chemical Surface Treatments on the Bond Strength of Resin-Matrix Ceramic Repaired with Resin Composite},
  journal = {European Journal of Dentistry},
  year = {2025},
  volume = {19},
  number = {01},
  pages = {165--172},
  doi = {10.1055/s-0044-1785531}
}
Kostenlos starten →