Effects of Repeated Thermo-Mechanical Processing on the Degradation Behavior of Bottle-Grade PET Under Controlled Conditions
Polymers · 2026-02-05 · 18 (3) · 416
DOI: 10.3390/polym18030416 ↗At a glance
Journal article in Polymers, published online on 2026-02-05. Written by Mária Straková and 12 co-authors. Institution: Institute of Natural and Synthetic Polymers, Faculty of Chemical and Food Technology, Slovak University of Technology, Radlinského 9, 812 37 Bratisla…. Cited 10 times so far (Crossref); 53 references. The full text is freely available (open access, CC BY 4.0).
Abstract (original language)
Mechanical recycling of polyethylene terephthalate (PET) is a key strategy for circular packaging applications; however, repeated thermo-mechanical processing leads to progressive polymer degradation. In this study, the effect of controlled repeated extrusion on the degradation behavior of bottle-grade PET was systematically investigated under laboratory conditions. Mechanical recycling was simulated using a co-rotating twin-screw extruder, where PET was subjected to up to four consecutive processing cycles corresponding to a cumulative residence time of 8 min. Progressive processing resulted in chain scission, reflected by a decrease in intrinsic viscosity from approximately 0.80 to 0.65 dL·g−1 and a corresponding reduction in molecular weight. Melt flow rate increased accordingly, indicating a gradual loss of melt strength. Differential scanning calorimetry revealed that the glass transition and melting temperatures remained nearly unchanged, while the degree of crystallinity increased from approximately 23.0% to 29.5%, accompanied by changes in crystallization behavior. These structural changes led to reduced ductility, with elongation at break decreasing from about 84% to 60%. Optical analysis showed systematic material darkening, and a strong linear correlation between lightness (L*) and intrinsic viscosity was observed. By isolating intrinsic thermo-mechanical degradation effects under controlled processing conditions, this study enables a clearer definition of realistic reuse limits for mechanically recycled bottle-grade PET. The results indicate that bottle-grade PET retains properties compatible with demanding applications only after a limited number of thermo-mechanical processing cycles, whereas further processing restricts its usability to less demanding applications such as fibers, films, and non-food packaging.
Subjects
Author keywords
Authors and institutions
- Institute of Natural and Synthetic Polymers, Faculty of Chemical and Food Technology, Slovak University of Technology, Radlinského 9, 812 37 Bratislava, Slovakia.
ORCID profiles: Jozef Feranc, Michal Ďurfina, Ján Kruželák, Pavol Alexy
Cite
APA
Straková, M., Hlaváčiková, S., Feranc, J., Suchánková, H., Kramárová, Z., Ďurfina, M., Omaníková, L., Hezaveh, M. R., Tomanová, K., Vanovčanová, Z., Kruželák, J., Alexy, P., & Plavec, R. (2026). Effects of Repeated Thermo-Mechanical Processing on the Degradation Behavior of Bottle-Grade PET Under Controlled Conditions. Polymers, 18(3), 416. https://doi.org/10.3390/polym18030416
Vancouver
Straková M, Hlaváčiková S, Feranc J, Suchánková H, Kramárová Z, Ďurfina M, et al. Effects of Repeated Thermo-Mechanical Processing on the Degradation Behavior of Bottle-Grade PET Under Controlled Conditions. Polymers. 2026;18(3):416. doi:10.3390/polym18030416
BibTeX
@article{Strakov2026,
author = {Straková, Mária and Hlaváčiková, Slávka and Feranc, Jozef and Suchánková, Henrieta and Kramárová, Zuzana and Ďurfina, Michal and Omaníková, Leona and Hezaveh, Mohammadhassan Rahnama and Tomanová, Katarína and Vanovčanová, Zuzana and Kruželák, Ján and Alexy, Pavol and Plavec, Roderik},
title = {Effects of Repeated Thermo-Mechanical Processing on the Degradation Behavior of Bottle-Grade PET Under Controlled Conditions},
journal = {Polymers},
year = {2026},
volume = {18},
number = {3},
pages = {416},
doi = {10.3390/polym18030416}
}
EUVIMED