Comparative Study on Microstructural Characteristics and Fatigue Performance of 10 mm Thick 5083-H111 Aluminum Alloy Plates Processed by Different Cutting Methods

Xin Li iD, Qiang Guo, Wanguo Li, Meijie Jia, Lei Wang

Materials · 01.11.2026 · 19 (21) · 4656

DOI: 10.3390/ma19214656 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 01.11.2026. Verfasst von Xin Li und 4 weiteren Autor:innen. Beteiligte Einrichtung: Key Laboratory of Automobile Materials, School of Materials Science and Engineering, Jilin University, Changchun 130022, China. Die Arbeit nennt 27 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Changchun rail transit equipment industry.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study evaluates the applicability of laser cutting to 10 mm thick 5083-H111 aluminum alloy plates by comparing fiber laser cutting, waterjet cutting, and mechanical grinding. The cut-edge morphology, microstructure, tensile properties, and fatigue behavior were systematically investigated, with particular emphasis on the effects of laser-induced thermal input on the heat-affected zone (HAZ), grain orientation, precipitates, and residual stress. A fatigue risk factor (Rf) was further introduced to quantify fatigue cracking susceptibility. At 1 × 107 cycles, the fatigue strengths of the mechanically ground specimen and the waterjet-cut, laser-cut without dross removal, and laser-cut with dross removal specimens were 119.18, 99.21, 60.19, and 67.64 MPa, respectively. Dross removal increased the fatigue strength of the laser-cut specimens by 12.38% by reducing local stress concentration, although their fatigue performance remained inferior to that of the other two processes. Periodic surface striations and heat-affected-zone degradation were identified as the primary causes of fatigue strength reduction. Fatigue cracks mainly initiated at dross roots, surface striations, and nearby defects in the laser-cut specimens. The laser-cut specimens exhibited the highest fatigue risk factor (Rf = 1.32), compared with 0.36 for waterjet cutting and 0.16 for mechanical grinding, corresponding to the lowest fatigue life.

Schlagwörter

Stichwörter der Autor:innen

5083-H111 aluminum alloyfatigue failure mechanismfatigue performancefatigue risk factorlaser cutting

Autor:innen und Institutionen

  • Key Laboratory of Automobile Materials, School of Materials Science and Engineering, Jilin University, Changchun 130022, China.
  • CRRC Changchun Railway Vehicles Co., Ltd., Changchun 130062, China.

ORCID-Profile: Xin Li

Förderung

  • Changchun rail transit equipment industry

Zitieren

APA

Li, X., Guo, Q., Li, W., Jia, M., & Wang, L. (2026). Comparative Study on Microstructural Characteristics and Fatigue Performance of 10 mm Thick 5083-H111 Aluminum Alloy Plates Processed by Different Cutting Methods. Materials, 19(21), 4656. https://doi.org/10.3390/ma19214656

Vancouver

Li X, Guo Q, Li W, Jia M, Wang L. Comparative Study on Microstructural Characteristics and Fatigue Performance of 10 mm Thick 5083-H111 Aluminum Alloy Plates Processed by Different Cutting Methods. Materials. 2026;19(21):4656. doi:10.3390/ma19214656

BibTeX
@article{Li2026,
  author = {Li, Xin and Guo, Qiang and Li, Wanguo and Jia, Meijie and Wang, Lei},
  title = {Comparative Study on Microstructural Characteristics and Fatigue Performance of 10 mm Thick 5083-H111 Aluminum Alloy Plates Processed by Different Cutting Methods},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {21},
  pages = {4656},
  doi = {10.3390/ma19214656}
}
Kostenlos starten →