Fachartikel in der Zeitschrift Materials, online erschienen am 28.03.2023. Verfasst von Branko Nečemer und 3 weiteren Autor:innen. Beteiligte Einrichtung: Faculty of Mechanical Engineering, University of Maribor, Smetanova 17, 2000 Maribor, Slovenia. Die Arbeit wurde bisher 9-mal zitiert (Crossref) und nennt 39 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Slovenian Research Agency.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study presents a comprehensive experimental investigation of the high-cycle fatigue (HCF) behaviour of the ductile aluminium alloy AA 5083-H111. The analysed specimens were fabricated in the rolling direction (RD) and transverse direction (TD). The HCF tests were performed in a load control (load ratio R = 0.1) at different loading levels under the loading frequency of 66 Hz up to the final failure of the specimen. The experimental results have shown that the S–N curves of the analysed Al-alloy consist of two linear curves with different slopes. Furthermore, RD-specimens demonstrated longer fatigue life if compared to TD-specimens. This difference was about 25% at the amplitude stress 65 MPa, where the average fatigue lives 276,551 cycles for RD-specimens, and 206,727 cycles for TD-specimens were obtained. Similar behaviour was also found for the lower amplitude stresses and fatigue lives between 106 and 108 cycles. The difference can be caused by large Al6(Mn,Fe) particles which are elongated in the rolling direction and cause higher stress concentrations in the case of TD-specimens. The micrography of the fractured surfaces has shown that the fracture characteristics were typical for the ductile materials and were similar for both specimen orientations.

Schlagwörter

Stichwörter der Autor:innen

aluminium alloysfracture analysishigh-cycle fatiguerolling direction

Autor:innen und Institutionen

  • Faculty of Mechanical Engineering, University of Maribor, Smetanova 17, 2000 Maribor, Slovenia.

ORCID-Profile: Franc Zupanič, Srečko Glodež

Förderung

  • Slovenian Research Agency

Zitieren

APA

Nečemer, B., Zupanič, F., Vuherer, T., & Glodež, S. (2023). High-Cycle Fatigue Behaviour of the Aluminium Alloy 5083-H111. Materials, 16(7), 2674. https://doi.org/10.3390/ma16072674

Vancouver

Nečemer B, Zupanič F, Vuherer T, Glodež S. High-Cycle Fatigue Behaviour of the Aluminium Alloy 5083-H111. Materials. 2023;16(7):2674. doi:10.3390/ma16072674

BibTeX
@article{Neemer2023,
  author = {Nečemer, Branko and Zupanič, Franc and Vuherer, Tomaž and Glodež, Srečko},
  title = {High-Cycle Fatigue Behaviour of the Aluminium Alloy 5083-H111},
  journal = {Materials},
  year = {2023},
  volume = {16},
  number = {7},
  pages = {2674},
  doi = {10.3390/ma16072674}
}
Kostenlos starten →