EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Thermomechanical Devulcanization of Highly Filled EPDM Rubber Waste: Process Optimization, Selectivity Assessment, and Preliminary Industrial Scale-Up

Pedro Veiga Rodrigues iD, Mateus Vieira Ribeiro, Ana Vera Machado iD

Materials · 29.10.2026 · 19 (21) · 4559

DOI: 10.3390/ma19214559 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 29.10.2026. Verfasst von Pedro Veiga Rodrigues und 2 weiteren Autor:innen. Beteiligte Einrichtung: Department of Polymer Engineering, Institute for Polymers and Composites (IPC), University of Minho, 4804-533 Guimarães, Portugal. Die Arbeit nennt 45 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Foundation for Science and Technology, FCT—Portuguese Foundation for Science and References.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Devulcanization of ethylene–propylene–diene monomer (EPDM) rubber is a promising strategy to improve the circularity of vulcanized automotive rubber waste. However, selective sulfur crosslink cleavage while preserving the polymer backbone remains challenging, particularly in highly filled industrial compounds. In this work, highly filled sulfur-cured EPDM waste from automotive sealing-profile production was thermomechanically devulcanized using 2,2′-dibenzamidodiphenyl disulfide (DBD) and hexadecylamine (HDA). Laboratory-scale experiments were performed in an internal mixer, followed by preliminary industrial-scale trials in a single-screw extruder. Crosslink density was determined using the Flory–Rehner equation with Kraus correction, and selectivity was assessed by Horikx analysis, supported by ATR-FTIR and rheometry. At laboratory scale, DBD showed optimal performance at 1 phr and 200 °C, reaching approximately 86% devulcanization, while higher DBD loading reduced efficiency. HDA reached approximately 85% devulcanization at 3 phr and 280 °C. Horikx analysis indicated preferential crosslink scission under optimized conditions, although mixed reclamation behavior was still observed. Industrial scale-up with 1 phr DBD at 200 °C achieved approximately 60% devulcanization, while HDA was less effective. The lower performance observed at the industrial scale highlights the challenges of translating laboratory-optimized conditions to industrial processing, although the individual contributions of specific processing parameters could not be determined from the available data.

Schlagwörter

Stichwörter der Autor:innen

DBDEPDM wasteHDAdevulcanization scale-upthermomechanical devulcanization

Autor:innen und Institutionen

  • Department of Polymer Engineering, Institute for Polymers and Composites (IPC), University of Minho, 4804-533 Guimarães, Portugal.

ORCID-Profile: Pedro Veiga Rodrigues, Ana Vera Machado

Förderung

  • Foundation for Science and Technology
  • FCT—Portuguese Foundation for Science and References

Zitieren

APA

Rodrigues, P. V., Ribeiro, M. V., & Machado, A. V. (2026). Thermomechanical Devulcanization of Highly Filled EPDM Rubber Waste: Process Optimization, Selectivity Assessment, and Preliminary Industrial Scale-Up. Materials, 19(21), 4559. https://doi.org/10.3390/ma19214559

Vancouver

Rodrigues PV, Ribeiro MV, Machado AV. Thermomechanical Devulcanization of Highly Filled EPDM Rubber Waste: Process Optimization, Selectivity Assessment, and Preliminary Industrial Scale-Up. Materials. 2026;19(21):4559. doi:10.3390/ma19214559

BibTeX
@article{Rodrigues2026,
  author = {Rodrigues, Pedro Veiga and Ribeiro, Mateus Vieira and Machado, Ana Vera},
  title = {Thermomechanical Devulcanization of Highly Filled EPDM Rubber Waste: Process Optimization, Selectivity Assessment, and Preliminary Industrial Scale-Up},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {21},
  pages = {4559},
  doi = {10.3390/ma19214559}
}
Kostenlos starten →