EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Investigation of Additive Friction Stir Deposition of Inconel 718: Mechanical Performance and Microstructural Evolution

Saeid Zavari iD, Selami Emanet iD, Huan Ding iD, Mahnaz Ensafi, Ehsan Bagheri, Carl Schmidt, Jeff Dulik, Shengmin Guo iD

Materials · 10.06.2026 · 19 (12) · 2482

DOI: 10.3390/ma19122482 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 10.06.2026. Verfasst von Saeid Zavari und 7 weiteren Autor:innen. Beteiligte Einrichtung: Department of Mechanical and Industrial Engineering, Louisiana State University, Baton Rouge, LA 70803, USA. Die Arbeit nennt 33 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: U.S. National Science Foundation, Louisiana Board of Regents, Center for Innovations in Structural Integrity Assurance (CISIA).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Additive friction stir deposition (AFSD) is a solid-state additive manufacturing process that enables the fabrication of fully dense metallic components without common fusion-related defects. Inconel 718, widely used in aerospace and energy sectors, requires high structural reliability; therefore, evaluating its response to AFSD is essential for advanced applications. This study investigates the effects of AFSD on IN718 by comparing the mechanical properties and microstructure of the as-deposited material with the feedstock condition. Tensile testing showed that the ultimate tensile strength (UTS) increased by 5% along the traverse direction, whereas elongation was reduced compared to the feedstock. In contrast, build-direction tensile specimens exhibited lower UTS and substantially reduced elongation, revealing mechanical anisotropy. Microhardness increased by 20%, consistent with substantial grain refinement from 11 µm to 3 µm due to dynamic recrystallization during deposition. X-ray diffraction (XRD) revealed no clearly detectable secondary phase formation after AFSD within the resolution limits of conventional XRD, suggesting that the increased hardness and traverse-direction strength can be partly explained by grain refinement. Elemental mapping detected oxygen-enriched Al/Ti regions at interlayer boundaries, which may contribute to the reduced build-direction ductility. Overall, AFSD refined the microstructure, enhanced hardness, and improved traverse-direction strength, while build-direction tensile testing revealed anisotropic mechanical behavior.

Schlagwörter

Stichwörter der Autor:innen

Inconel 718MELDadditive friction stir deposition (AFSD)mechanical propertiesmicrostructural analysisnickel-based super alloys

Autor:innen und Institutionen

  • Department of Mechanical and Industrial Engineering, Louisiana State University, Baton Rouge, LA 70803, USA.
  • Bechtel Plant Machinery, Inc. (BPMI), 3500 Technology Drive, Monroeville, PA 15146, USA.

ORCID-Profile: Saeid Zavari, Selami Emanet, Huan Ding, Shengmin Guo

Förderung

  • U.S. National Science Foundation
  • Louisiana Board of Regents
  • Center for Innovations in Structural Integrity Assurance (CISIA)
  • Bechtel Plant Machinery, Inc. through SAM.gov Open Solicitation FMP-NNL-0027 "Accelerated Ship Construction".
  • US National Science Foundation
  • Bechtel Plant Machinery, Inc.

Zitieren

APA

Zavari, S., Emanet, S., Ding, H., Ensafi, M., Bagheri, E., Schmidt, C., Dulik, J., & Guo, S. (2026). Investigation of Additive Friction Stir Deposition of Inconel 718: Mechanical Performance and Microstructural Evolution. Materials, 19(12), 2482. https://doi.org/10.3390/ma19122482

Vancouver

Zavari S, Emanet S, Ding H, Ensafi M, Bagheri E, Schmidt C, et al. Investigation of Additive Friction Stir Deposition of Inconel 718: Mechanical Performance and Microstructural Evolution. Materials. 2026;19(12):2482. doi:10.3390/ma19122482

BibTeX
@article{Zavari2026,
  author = {Zavari, Saeid and Emanet, Selami and Ding, Huan and Ensafi, Mahnaz and Bagheri, Ehsan and Schmidt, Carl and Dulik, Jeff and Guo, Shengmin},
  title = {Investigation of Additive Friction Stir Deposition of Inconel 718: Mechanical Performance and Microstructural Evolution},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {12},
  pages = {2482},
  doi = {10.3390/ma19122482}
}
Kostenlos starten →