Abstract (Originalsprache)
Objectives
Studies have shown that nanoparticles can impart beneficial properties when integrated into resin composites; however, it remains unclear how this affects shear bond strength. This study aimed to evaluate the effects of composite formulation and zein-coated magnesium oxide nanoparticle (zMgO NP) concentration on shear bond strength (SBS) and failure mode following thermocycling.
Methods
A total of 180 extracted human molars were randomly allocated among four composite formulations and three zMgO NP concentrations (0%, 0.5%, and 1%; n = 15). Composite cylinders were bonded to prepared dentin surfaces and thermocycled for 10,000 cycles between 5 °C and 55 °C. SBS was analyzed using two-way ANOVA and post hoc multiple comparisons with Tukey’s test. Failure modes were assessed stereomicroscopically and analyzed using the chi-square test.
Results
The SBS of the modified composites in all groups significantly increased, with the 0.5% zMgO NP groups exhibiting the highest SBS. The 0.5% zMgO NPs N-Ceram group had the highest SBS overall. The unmodified Z350 composite exhibited the highest adhesive failure, while the control N-Flow composite demonstrated the highest cohesive failure. The modified conventional and flowable composites showed initially lower adhesive failure, which increased progressively as zMgO NPs increased. The bulk-fill composite initially showed higher adhesive failure, with the 0.5% group demonstrating lower adhesive failure and the 1% group exhibiting increased adhesive failure.
Conclusions
Adding zMgO NPs to resin composites improved SBS after thermocycling, with material- and concentration-dependent differences in failure-mode analysis. Further validation studies are needed to verify clinical viability.
Zitieren
APA
Naguib, G. H., Aljawi, R., Alqarni, S., Alsharif, D., Mazhar, J., Alnowaiser, A., & Hamed, M. T. (2026). Effect of Zein-Coated Magnesium Oxide Nanoparticle Incorporation on the Shear Bond Strength of Different Resin Composites After Thermocycling. Bioengineering, 13(11), 1353. https://doi.org/10.3390/bioengineering13111353
Vancouver
Naguib GH, Aljawi R, Alqarni S, Alsharif D, Mazhar J, Alnowaiser A, et al. Effect of Zein-Coated Magnesium Oxide Nanoparticle Incorporation on the Shear Bond Strength of Different Resin Composites After Thermocycling. Bioengineering. 2026;13(11):1353. doi:10.3390/bioengineering13111353
BibTeX
@article{Naguib2026,
author = {Naguib, Ghada H. and Aljawi, Rabab and Alqarni, Sarah and Alsharif, Dina and Mazhar, Jumana and Alnowaiser, Abeer and Hamed, Mohamed T.},
title = {Effect of Zein-Coated Magnesium Oxide Nanoparticle Incorporation on the Shear Bond Strength of Different Resin Composites After Thermocycling},
journal = {Bioengineering},
year = {2026},
volume = {13},
number = {11},
pages = {1353},
doi = {10.3390/bioengineering13111353}
}
EUVIMED