Flexural strength of repaired denture base materials manufactured for the CAD-CAM technique

Şebnem Özatik iD, Canan Bural iD

Journal of Oral Science · 2024

DOI: 10.2334/josnusd.23-0275 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Oral Science, 2024. Verfasst von Şebnem Özatik und 1 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthodontics, Faculty of Dentistry, Istanbul University. Hauptthemen laut MEDLINE: Flexural Strength, Dental Materials. Die Arbeit wurde bisher 4-mal zitiert (Crossref) und nennt 40 Literaturangaben. Gefördert von: Scientific Research Projects Coordination Unit of Istanbul University.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

PURPOSE: To evaluate the flexural properties of repaired poly(methylmethacrylate) (PMMA) denture base materials for computer-aided design/computer-aided manufacturing (CAD-CAM) and to compare them with heat-activated polymerized PMMA. METHODS: A total of 288 specimens (65 × 10 × 2.5 mm) were prepared using both CAD-CAM and conventional blocks and repaired using autopolymerizing and visible-light polymerizing (VLC) materials. Microwave energy, water storage and hydroflask polymerization were applied as additional post-polymerization cycles after the repair process. The flexural strength (FS) of the specimens was evaluated using the three-point bending test. Data were evaluated statistically using 2-way ANOVA followed by Bonferroni's correction to determine the significance of differences between the groups (P ≤ 0.05). RESULTS: The FS of the denture base materials for CAD-CAM was significantly higher than that for the heat-activated group (P ≤ 0.05). The FS was significantly highest when microwave energy was used for the post-polymerization cycle. The FS values for all groups repaired with VLC resin were significantly lower than for the autopolymerization group (P ≤ 0.05). CONCLUSION: The flexural properties of denture base materials for CAD-CAM repaired using autopolymerizing acrylic resins can recover by 50-70%. Additional post-polymerization cycles for autopolymerizing repair resin can be suggested to improve the clinical service properties of repaired dentures.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

Flexural StrengthDental MaterialsPolymethyl MethacrylateDenture BasesMaterials TestingAcrylic ResinsComputer-Aided DesignDenture RepairSurface Properties

Stichwörter der Autor:innen

CAD-CAMautopolymerizing acrylic resinpolymerization cyclerepairvisible-light polymerizing resin

Substanzen

Dental MaterialsPolymethyl MethacrylateAcrylic Resins

Autor:innen und Institutionen

  • Department of Prosthodontics, Faculty of Dentistry, Istanbul University.

ORCID-Profile: Şebnem Özatik, Canan Bural

Förderung

  • Scientific Research Projects Coordination Unit of Istanbul University

Zitieren

APA

Özatik, Ş., & Bural, C. (2024). Flexural strength of repaired denture base materials manufactured for the CAD-CAM technique. Journal of Oral Science. https://doi.org/10.2334/josnusd.23-0275

Vancouver

Özatik Ş, Bural C. Flexural strength of repaired denture base materials manufactured for the CAD-CAM technique. Journal of Oral Science. 2024. doi:10.2334/josnusd.23-0275

BibTeX
@article{zatik2024,
  author = {Özatik, Şebnem and Bural, Canan},
  title = {Flexural strength of repaired denture base materials manufactured for the CAD-CAM technique},
  journal = {Journal of Oral Science},
  year = {2024},
  doi = {10.2334/josnusd.23-0275}
}
Kostenlos starten →