ENSURING QUALITY AND ACCURACY OF FINISHING AEROSPACE PARTS USING FREE ABRASIVE

S.O. Ulanov, O.Ya. Kachan

Kosmìčna nauka ì tehnologìâ · 29.08.2026 · 32 (4) · 041-047

DOI: 10.15407/knit2026.04.041 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Kosmìčna nauka ì tehnologìâ, online erschienen am 29.08.2026. Verfasst von S.O. Ulanov und 1 weiteren Autor:innen. Die Arbeit nennt 26 Literaturangaben.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Th e paper investigates the process of intensifying the fi nishing treatment of full-scale gas turbine engine compressor disks made of diffi cult-to-machine titanium (VT3-1, VT9) and heat-resistant (EI698-VD) alloys in an abrasive fl uidized bed (AFB). Th e problem of replacing labor-intensive manual operations with automated methods to ensure high fatigue strength and reliability of highly loaded complex-profi le parts is considered. Th e regularities in the eff ects of abrasive medium composition and low-frequency vibrations on process productivity and surface layer quality have been experimentally established. It is shown that using a multicomponent mixture of green silicon carbide abrasive grains of 63C50 and 63C25 fractions at an equal mass ratio reduces machining time by 1.5 times compared to the base single-fraction abrasive. Additional application of low-frequency vibrations at 20...55 Hz and an amplitude of 2... 3 mm to the workpiece ensures a further reduction in machining time. It has been establ ished that the proposed method guarantees the preservation of the geometric dimensions of complex-profi le parts within the drawing tolerances with minimal material removal on the disk web (0.01...0.04 mm). Th e process ensures uniform rounding of sharp edges along the blade slot contour with a radius of 0.2...0.3 mm and eff ective polishing of the disk web to a surface roughness of Ra = 0.63...1.25 μm. It is experimentally proven that free abrasive machining does not lead to the degradation of the physical and mechanical state of the surface: the microhardness remains unchanged, and the favorable compressive residual stresses formed during the previous stages of fi nish turning are preserved at the level of 450...550 MPa at a depth of up to 140 μm. It is noted that to eliminate the side eff ect of hole-chamfer erosion on the disk web, the technological process should include their preliminary protection or postpone the chamfering operation to the fi nal stage.

Zitieren

APA

Ulanov, S., & Kachan, O. (2026). ENSURING QUALITY AND ACCURACY OF FINISHING AEROSPACE PARTS USING FREE ABRASIVE. Kosmìčna nauka ì tehnologìâ, 32(4), 041-047. https://doi.org/10.15407/knit2026.04.041

Vancouver

Ulanov S, Kachan O. ENSURING QUALITY AND ACCURACY OF FINISHING AEROSPACE PARTS USING FREE ABRASIVE. Kosmìčna nauka ì tehnologìâ. 2026;32(4):041-047. doi:10.15407/knit2026.04.041

BibTeX
@article{Ulanov2026,
  author = {Ulanov, S.O. and Kachan, O.Ya.},
  title = {ENSURING QUALITY AND ACCURACY OF FINISHING AEROSPACE PARTS USING FREE ABRASIVE},
  journal = {Kosmìčna nauka ì tehnologìâ},
  year = {2026},
  volume = {32},
  number = {4},
  pages = {041--047},
  doi = {10.15407/knit2026.04.041}
}
Kostenlos starten →