Provides Efficient Shear Bond Strength and Durability Between Lithium Disilicate Glass-ceramic and Resin Cement: A Potential Alternative to the Conventional Hydrofluoric Acid Protocal

Top Chitkraisorn, Nontawat Chuinsiri, Chawin Aungkatawiwat, Weerachai Singhatanadgit, Terawat Tosiriwatanapong

Oral Sciences Reports · 15.11.2024 · 45 (3) · 45-51

DOI: 10.12982/osr.2024.035 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Oral Sciences Reports, online erschienen am 15.11.2024. Verfasst von Top Chitkraisorn und 4 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Objectives

This study investigated the effects of two surface treatment protocols on the shear bond strength, bond durability, and failure mode at the interface between lithium disilicate glass-ceramic and resin cement. The protocols compared were a self-etching ceramic primer and the conventional hydrofluoric acid (HF) etching followed by silane.

Methods

Fifty lithium disilicate specimens were randomly divided into five surface treatment groups (n=10 each). A control group received no treatment. The remaining 4groups included: 5% HF etch with Monobond Plus thermocycled and non-thermocycled, Monobond Etch & Prime (MEP), thermocycled and non-thermocycled. Microshear bond strength (microSBS) was assessed before and after thermocycling to evaluate bond durability. Failure modes (adhesive, mixed, cohesive in resin/ceramic) were recorded under a stereomicroscope.

Results

Both surface treatment protocols exhibited comparable microSBS for both pre- and post-thermocycling results. Moreover, bone durability obtained from the two treatment protocols seemed to be comparable. Most groups displayed adhesive/mixed failures. Notably, the self-etching ceramic primer group showed cohesive failure in half of the specimens initially, persisting in 20% after thermal aging.

Conclusions

Compared with the conventional HF protocol, the self-etching ceramic primer protocol provided similar microSBS and bond durability between lithium disilicate glass-ceramic and resin cement. The data suggest a self-etching ceramic primer is a viable option for the conventional HF protocol in bonding to glass-ceramic, minimizing the HF hazard and simplifying the clinical procedure.

Zitieren

APA

Chitkraisorn, T., Chuinsiri, N., Aungkatawiwat, C., Singhatanadgit, W., & Tosiriwatanapong, T. (2024). Provides Efficient Shear Bond Strength and Durability Between Lithium Disilicate Glass-ceramic and Resin Cement: A Potential Alternative to the Conventional Hydrofluoric Acid Protocal. Oral Sciences Reports, 45(3), 45-51. https://doi.org/10.12982/osr.2024.035

Vancouver

Chitkraisorn T, Chuinsiri N, Aungkatawiwat C, Singhatanadgit W, Tosiriwatanapong T. Provides Efficient Shear Bond Strength and Durability Between Lithium Disilicate Glass-ceramic and Resin Cement: A Potential Alternative to the Conventional Hydrofluoric Acid Protocal. Oral Sciences Reports. 2024;45(3):45-51. doi:10.12982/osr.2024.035

BibTeX
@article{Chitkraisorn2024,
  author = {Chitkraisorn, Top and Chuinsiri, Nontawat and Aungkatawiwat, Chawin and Singhatanadgit, Weerachai and Tosiriwatanapong, Terawat},
  title = {Provides Efficient Shear Bond Strength and Durability Between Lithium Disilicate Glass-ceramic and Resin Cement: A Potential Alternative to the Conventional Hydrofluoric Acid Protocal},
  journal = {Oral Sciences Reports},
  year = {2024},
  volume = {45},
  number = {3},
  pages = {45--51},
  doi = {10.12982/osr.2024.035}
}
Kostenlos starten →