EUVIMEDEUVIMED entdecken
Crossref

Experimental evaluation of tensile tests of fused deposition modeling printed-hole and drilled-hole polylactic acid

Ender Emir

Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering · 18.11.2026

DOI: 10.1177/09544089261508383 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering, online erschienen am 18.11.2026. Verfasst von Ender Emir. Die Arbeit nennt 37 Literaturangaben.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study experimentally investigated the effects of raster angle, printing temperature, and hole-generation method on the tensile behavior of fused deposition modeling-printed polylactic acid specimens containing through-holes. Modified ASTM D638 Type IV specimens were produced at raster angles of 0°, ±45°, and 90° and printing temperatures of 190, 210, and 230 °C, with holes either incorporated during printing or produced subsequently by drilling. Tensile tests were performed to determine the maximum force ( F max ), ultimate tensile strength, energy absorption, and elastic modulus ( E ), while entrance and exit delamination factors were evaluated for drilled specimens. Raster angle was the dominant factor of mechanical responses, with a strong statistically significant effect on ultimate tensile strength, energy absorption, and E (partial η 2 = 0.970, 0.998, and 0.822, respectively; all p < 0.001). Printing temperature significantly affected ultimate tensile strength ( p < 0.001), with the principal improvement occurring between 190 and 210 °C; increasing the temperature further to 230 °C did not improve tensile strength. A significant raster angle × hole-generation method interaction was observed for ultimate tensile strength, energy absorption, and E (all p < 0.001). Within-angle comparisons showed that drilling increased ultimate tensile strength and energy absorption at 0° and 45°, whereas both responses decreased at 90°. Exit delamination was significantly greater than entrance delamination ( p < 0.001), but neither delamination factor showed a significant association with the mechanical responses.

Zitieren

APA

Emir, E. (2026). Experimental evaluation of tensile tests of fused deposition modeling printed-hole and drilled-hole polylactic acid. Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering. https://doi.org/10.1177/09544089261508383

Vancouver

Emir E. Experimental evaluation of tensile tests of fused deposition modeling printed-hole and drilled-hole polylactic acid. Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering. 2026. doi:10.1177/09544089261508383

BibTeX
@article{Emir2026,
  author = {Emir, Ender},
  title = {Experimental evaluation of tensile tests of fused deposition modeling printed-hole and drilled-hole polylactic acid},
  journal = {Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering},
  year = {2026},
  doi = {10.1177/09544089261508383}
}
Kostenlos starten →