EUVIMEDObjevte EUVIMED
Crossref

Shear Bond Strength of Five Different Repair Systems to Three Different Ceramic Materials

Martin Janda, Evaggelia Papia, Christel Larsson

The International Journal of Prosthodontics · 2025

DOI: 10.11607/ijp.9179 ↗

At a glance

Journal article in The International Journal of Prosthodontics, 2025. Written by Martin Janda and 2 co-authors. Major MEDLINE topics: Dental Bonding, Dental Porcelain, Ceramics, Dental Materials. Cited 1 times so far (Crossref).

AbstraktSubjectsBibliografické údajeCiteRelated studies

Abstract (original language)

Purpose

To investigate the shear bond strength of composite resin in five different ceramic repair systems for three different ceramic materials. Materials and Methods: A total of 225 monolithic zirconia (Zr), lithium disilicate (LDS), and cobalt-chromium (CoCr) specimens with feldspathic porcelain (FP) veneer were fabricated (N = 75 per material). The specimens underwent thermocycling and were randomly divided into five groups for the following intraoral repair systems (n = 15): (1) Clearfil Ceramic Primer Plus, Kuraray Noritake; (2) iBond Intraoral Repair Kit, Kulzer; (3) VOCO Cimara, VOCO Dental; (4) Ceramic Repair System Kit, Ivoclar Vivadent; and (5) Ultradent Porcelain Repair Kit, Ultradent Products. After surface conditioning, composite was applied using a cylindrical mold, and a second round of thermocycling was performed. Each specimen was then subjected to shear load until failure. Microshear bond strength was compared using one-way ANOVA (Tukey test, α < .05).

Results

The type of porcelain repair kit significantly affected the shear bond strength. For Zr, the repair systems from Kulzer and VOCO had significantly higher shear bond strength than the other systems (P < .001), without significant difference between Kulzer and VOCO. For the LDS and CoCr with FP, hydrofluoric acid had the highest shear bond strength (P < .001).

Conclusions

For zirconia, a 10-methacryloyloxydecyl dihydrogen phosphate (10-MDP) system should be used. The results also suggest that a cleaning bur may be beneficial. For glass-based ceramics and FP, etching with hydrofluoric acid remains the method of choice.

Subjects

MeSH terms (MEDLINE)

Dental BondingDental PorcelainCeramicsDental MaterialsDental Restoration RepairDental Prosthesis RepairShear StrengthMaterials TestingZirconiumComposite ResinsDental Stress AnalysisDental VeneersSurface PropertiesResin Cements

Substances

Dental PorcelainZirconiumzirconium oxideComposite Resinslithia disilicateDental MaterialsResin Cements

Cite

APA

Janda, M., Papia, E., & Larsson, C. (2025). Shear Bond Strength of Five Different Repair Systems to Three Different Ceramic Materials. The International Journal of Prosthodontics. https://doi.org/10.11607/ijp.9179

Vancouver

Janda M, Papia E, Larsson C. Shear Bond Strength of Five Different Repair Systems to Three Different Ceramic Materials. The International Journal of Prosthodontics. 2025. doi:10.11607/ijp.9179

BibTeX
@article{Janda2025,
  author = {Janda, Martin and Papia, Evaggelia and Larsson, Christel},
  title = {Shear Bond Strength of Five Different Repair Systems to Three Different Ceramic Materials},
  journal = {The International Journal of Prosthodontics},
  year = {2025},
  doi = {10.11607/ijp.9179}
}
Start for free →