Effect of Surface Treatment with Alkaline Agents at Two Different Temperatures on Microshear Bond Strength of Zirconia to Composite Resin
BioMed Research International · 2024
DOI: 10.1155/2024/7720286 ↗Kurz gefasst
Fachartikel in der Zeitschrift BioMed Research International, 2024. Verfasst von Faeze Jamali Zavare und 3 weiteren Autor:innen. Beteiligte Einrichtung: Department of Operative Dentistry, School of Dentistry, Shahid Beheshti University of Medical Sciences, Tehran Postcode: 1983969411, Iran. Hauptthemen laut MEDLINE: Composite Resins, Dental Bonding. Die Arbeit wurde bisher 3-mal zitiert (Crossref) und nennt 23 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
Background
Zirconia, with its excellent mechanical properties, has become a popular choice for esthetic and durable restorations due to the increasing demand of patients. It has overcome most of the limitations of all ceramic restorations. However, bonding to zirconia remains a challenge.
Objectives
This study is aimed at assessing the effect of surface treatment with alkaline agents at two different temperatures on microshear bond strength (μSBS) of zirconia to composite resin. Materials and Methods. This in vitro, experimental study was conducted on zirconia blocks measuring 2 × 4 × 8 mm. The blocks were sandblasted with alumina powder and randomly assigned to 5 groups ( n = 16 each). The blocks in groups 1 and 2 underwent surface treatment with sodium hydroxide (NaOH) and groups 3 and 4 with zirconium hydroxide (Zr(OH)4) at room temperature and 70°C. Group 5 served as the control group and did not receive any surface treatment. After the application of bonding agent and its light-curing, composite cylinders in plastic tubes were bonded to the surface of each block and cured. After incubation, they underwent μSBS test. Data were analyzed by one-way ANOVA and Tukey’s test ( alpha = 0.05 ).
Results
The μSBS was significantly higher in all intervention groups than that in the control group ( P < 0.05 ). The μSBS in Zr(OH)4 groups was significantly higher than that in NaOH groups ( P < 0.05 ). The mean μSBS of heated groups was slightly, but not significantly, higher than the corresponding room temperature groups ( P > 0.05 ).
Conclusion
Surface treatment of zirconia with NaOH and Zr(OH)4 alkaline agents can increase its μSBS to composite resin; Zr(OH)4 was significantly more effective than NAOH for this purpose, but heating did not have a significant effect on μSBS.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Substanzen
Autor:innen und Institutionen
- Department of Operative Dentistry, School of Dentistry, Shahid Beheshti University of Medical Sciences, Tehran Postcode: 1983969411, Iran.
- School of Dentistry, Shahid Beheshti University of Medical Sciences, Tehran Postcode: 1983969411, Iran.
ORCID-Profile: Faeze Jamali Zavare, Seyed Reza Khosravani, Moein Sabzivand, Narges Panahandeh
Zitieren
APA
Zavare, F. J., Khosravani, S. R., Sabzivand, M., & Panahandeh, N. (2024). Effect of Surface Treatment with Alkaline Agents at Two Different Temperatures on Microshear Bond Strength of Zirconia to Composite Resin. BioMed Research International. https://doi.org/10.1155/2024/7720286
Vancouver
Zavare FJ, Khosravani SR, Sabzivand M, Panahandeh N. Effect of Surface Treatment with Alkaline Agents at Two Different Temperatures on Microshear Bond Strength of Zirconia to Composite Resin. BioMed Research International. 2024. doi:10.1155/2024/7720286
BibTeX
@article{Zavare2024,
author = {Zavare, Faeze Jamali and Khosravani, Seyed Reza and Sabzivand, Moein and Panahandeh, Narges},
title = {Effect of Surface Treatment with Alkaline Agents at Two Different Temperatures on Microshear Bond Strength of Zirconia to Composite Resin},
journal = {BioMed Research International},
year = {2024},
doi = {10.1155/2024/7720286}
}
EUVIMED