Fachartikel in der Zeitschrift Journal of Prosthodontics, online erschienen am 29.05.2026. Verfasst von Engin Sacu und 5 weiteren Autor:innen. Beteiligte Einrichtung: Department of Restorative Dentistry, Faculty of Dentistry, Kocaeli University, Kocaeli, Turkey. Die Arbeit nennt 39 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Scientific Research Projects (BAP) Unit of Kocaeli University.
Abstract (Originalsprache)
Purpose
This study aimed to compare the effects of surface treatment protocols on the surface roughness and shear bond strength (SBS) of a three‐dimensional (3D)‐printable resin for definitive crowns. Materials and Methods A 3D‐printable resin for definitive crowns (Saremco Print Crowntec) was used to produce 168 specimens (10 × 10 × 2 mm 3 ) using liquid crystal display (LCD)‐based technology. Specimens were allocated to seven surface treatment groups ( n = 24/group): control, Al 2 O 3 air abrasion (110 µm, 50 µm), 9% hydrofluoric acid (HF) etching (1 and 3 min), and CO 2 laser treatment with parallel and grid patterns. Each group included 12 specimens with primer and 12 specimens without primer. Dual‐cure cement was applied via cylindrical molds (Ø2.38 × 3 mm). SBS tests were conducted. Data were analyzed using two‐way ANOVA and the Tukey test ( p < 0.05).
Results
Surface treatments significantly affected SBS ( p < 0.001). The highest SBS was with 110‐µm Al 2 O 3 air abrasion (14.05 ± 3.78 MPa), followed by CO 2 laser with parallel lines (11.86 ± 5.51 MPa). The 1‐min HF etching (9.47 ± 4.04 MPa) and the control group (7.08 ± 2.98 MPa) showed low SBS. The primer application did not significantly affect SBS. A weak positive correlation was found between SBS and surface roughness ( r = 0.297, p = 0.006).
Conclusions
Air abrasion with 110‐µm Al 2 O 3 provided the highest bond strength for 3D‐printed restorations. CO 2 laser with parallel line patterns was an alternative. Under the tested conditions, 1‐min HF etching showed low bond strength, whereas a 3‐min application resulted in improved outcomes. Surface roughness appears to aid bonding, but is not sufficient alone.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Department of Restorative Dentistry, Faculty of Dentistry, Kocaeli University, Kocaeli, Turkey.
- Faculty of Aeronautics and Astronautics, Kocaeli University, Kocaeli, Turkey.
ORCID-Profile: Engin Sacu, Mehmet Can Ararat, Sinan Fidan, Satılmış Ürgün, Mustafa Özgür Bora, Neslihan Tekce
Förderung
- Scientific Research Projects (BAP) Unit of Kocaeli University
Zitieren
APA
Sacu, E., Ararat, M. C., Fidan, S., Ürgün, S., Bora, M. Ö., & Tekce, N. (2026). Comparison of surface treatment protocols for a 3D‐printable resin for definitive crowns: Effects on surface roughness and bonding performance. Journal of Prosthodontics. https://doi.org/10.1111/jopr.70173
Vancouver
Sacu E, Ararat MC, Fidan S, Ürgün S, Bora MÖ, Tekce N. Comparison of surface treatment protocols for a 3D‐printable resin for definitive crowns: Effects on surface roughness and bonding performance. Journal of Prosthodontics. 2026. doi:10.1111/jopr.70173
BibTeX
@article{Sacu2026,
author = {Sacu, Engin and Ararat, Mehmet Can and Fidan, Sinan and Ürgün, Satılmış and Bora, Mustafa Özgür and Tekce, Neslihan},
title = {Comparison of surface treatment protocols for a 3D‐printable resin for definitive crowns: Effects on surface roughness and bonding performance},
journal = {Journal of Prosthodontics},
year = {2026},
doi = {10.1111/jopr.70173}
}
EUVIMED