Fachartikel in der Zeitschrift Journal of Prosthodontics, 2025. Verfasst von Maram A AlGhamdi und 9 weiteren Autor:innen. Beteiligte Einrichtung: Department of Substitutive Dental Sciences, College of Dentistry, Imam Abdulrahman Bin Faisal University, Dammam, Saudi Arabia. Hauptthemen laut MEDLINE: Zirconium, Silicon Dioxide, Printing, Three-Dimensional, Nanocomposites. Die Arbeit wurde bisher 16-mal zitiert (Crossref) und nennt 29 Literaturangaben.
Abstract (Originalsprache)
Purpose
The aim of this study was to investigate and compare the influence of zirconium dioxide nanoparticles (ZrO 2 NPs) and silicon dioxide nanoparticles (SiO 2 NPs) addition and printing orientation on the flexural strength (FS) of provisional three‐dimensional (3D) printing resins undergoing thermal cycling (TC).
Methods
Three dimensional‐printed resin (NextDent C&B MFH) was used to fabricate 300 bar‐shaped specimens (25 × 2 × 2 mm 3 ). The ZrO 2 NPs and SiO 2 NPs specimens were divided into two groups, then subdivided into three groups, based on the nanoparticle concentration (i.e., 0 wt% (original group), 0.5 wt%, and 1 wt%). Each concentration was printed in three printing orientations (0°, 45°, and 90°). The printed specimens were exposed to 5000 cycles of TC, followed by a three‐point bending test to assess the FS. Fracture surface analysis was conducted by using a scanning electron microscope (SEM). For data analysis, ANOVA and Tukey's post hoc were utilized ( α = 0.05).
Results
Compared to the original material, the addition of ZrO 2 NPs and SiO 2 NPs had a significantly positive impact on the FS, ( P > 0.001). After TC, the FS of the original group decreased significantly and had the lowest value. The highest FS value was observed in 1% ZrO 2 NPs at 0°. Regardless of the nanoparticle concentration, the 0° orientation consistently showed a higher FS, compared to the 45° and 90° orientations. At all orientations (i.e., 0°, 45°, and 90°), the FS significantly increased with the addition of NPs, compared with that of the original material ( P > 0.001). TC had a significantly negative effect on the FS of the unmodified groups. However, no significant differences existed in FS among the modified groups after TC.
Conclusion
The addition of SiO 2 NPs and ZrO 2 NPs increased the FS of the 3D‐printed provisional resin. Regardless of the nanoparticle concentration, the 0° orientation had the higher FS. TC had an effect on the original resin, whereas it had no significant effect on the nanoparticle‐modified resins. In clinical practice, 3D‐printed provisional nanocomposite resins printed at the 0° orientation could be recommended for long‐term dental provisional restorations.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Department of Substitutive Dental Sciences, College of Dentistry, Imam Abdulrahman Bin Faisal University, Dammam, Saudi Arabia.
- College of Dentistry, Imam Abdulrahman Bin Faisal University, Dammam, Saudi Arabia.
- Department of Preventive Dental Sciences, College of Dentistry, Imam Abdulrahman Bin Faisal University, Dammam, Saudi Arabia.
- Department of Biophysics, Institute for Research and Medical Consultations (IRMC), Imam Abdulrahman Bin Faisal University, Dammam, Saudi Arabia.
- Department of Dental Education, College of Dentistry, Imam Abdulrahman Bin Faisal University, Dammam, Saudi Arabia.
ORCID-Profile: Maram A AlGhamdi, Mohammed M Gad
Zitieren
APA
AlGhamdi, M. A., Alatiyyah, F. M., Dawood, Z. H. A., Alshaikhnasser, F. Y., Almedarham, R. F., Alboryh, S. Y., Elakel, A., Akhtar, S., Khan, S. Q., & Gad, M. M. (2025). Flexural strength of 3D‐printed nanocomposite provisional resins: Impact of SiO 2 and ZrO 2 nanoparticles and printing orientations in vitro. Journal of Prosthodontics. https://doi.org/10.1111/jopr.13829
Vancouver
AlGhamdi MA, Alatiyyah FM, Dawood ZHA, Alshaikhnasser FY, Almedarham RF, Alboryh SY, et al. Flexural strength of 3D‐printed nanocomposite provisional resins: Impact of SiO 2 and ZrO 2 nanoparticles and printing orientations in vitro. Journal of Prosthodontics. 2025. doi:10.1111/jopr.13829
BibTeX
@article{AlGhamdi2025,
author = {AlGhamdi, Maram A and Alatiyyah, Fatimah M and Dawood, Zainab H Al and Alshaikhnasser, Farah Y and Almedarham, Rawan F and Alboryh, Shaymaa Y and Elakel, Ahmed and Akhtar, Sultan and Khan, Soban Q and Gad, Mohammed M},
title = {Flexural strength of 3D‐printed nanocomposite provisional resins: Impact of SiO 2 and ZrO 2 nanoparticles and printing orientations in vitro},
journal = {Journal of Prosthodontics},
year = {2025},
doi = {10.1111/jopr.13829}
}
EUVIMED