Influence of Airborne‐Particle Abrasion and Thermal Cycling on Enamel Bond Strength and Roughness of Lithium Disilicate Treated With a Self‐Etching Ceramic Primer
Journal of Esthetic and Restorative Dentistry · 2026-07 · 38 (7) · 1367-1375
DOI: 10.1111/jerd.70132 ↗At a glance
Journal article in Journal of Esthetic and Restorative Dentistry, published online on 2026-02-23. Written by Gabriel Freitas Pereira and 4 co-authors. Institution: Department of Restorative Dentistry, Faculty of Pharmacy, Dentistry and Nursing, Federal University of Ceará, Fortaleza, Ceará, Brazil. Major MEDLINE topics: Dental Porcelain, Dental Enamel, Dental Bonding, Dental Etching. Cited 2 times so far (Crossref); 56 references. The full text is freely available (open access, CC BY 4.0).
Abstract (original language)
Objective
This in vitro study investigated the effect of a self‐etching ceramic primer (Monobond Etch & Prime [MEP]), with or without aluminum oxide airborne‐particle abrasion, on the surface roughness, and microtensile bond strength (μTBS) of lithium disilicate bonded to enamel, compared with the conventional hydrofluoric acid plus silane (HF + S). Materials and Methods Lithium disilicate specimens (10 × 10 × 4 mm) were assigned to four groups: HF + S airborne‐particle abraded (HF + S[a]), HF + S polished (HF + S[p]), MEP airborne‐particle abraded (MEP[a]), and MEP polished (MEP[p]). Surface roughness (Δ S a ) was assessed after conditioning, and specimens were bonded to bovine enamel with resin cement. μTBS was tested before and after thermo cycling (10,000 cycles, 5°C/55°C).
Results
Airborne‐particle abrasion significantly increased Δ S a (HF + S[a]: 1.16 ± 0.12 μm; MEP[a]: 0.85 ± 0.02 μm) compared to polished specimens (HF + S[p]: 0.47 ± 0.04 μm; MEP[p]: 0.38 ± 0.04 μm). HF + S and MEP performed similarly in all conditions ( p > 0.05). Airborne‐particle abraded surfaces consistently exhibited higher μTBS than polished ones ( p < 0.05). Thermo cycling significantly reduced μTBS in all groups. Mixed and cohesive failures predominated before thermo cycling, whereas adhesive failures increased after.
Conclusion
MEP and HF + S demonstrated comparable bonding to enamel. Airborne‐particle abrasion enhanced both surface roughness and μTBS, regardless of conditioning strategy. Although thermo cycling reduced adhesion in all groups, the decline was similar across treatments.
Subjects
MeSH terms (MEDLINE)
Author keywords
Substances
Authors and institutions
- Department of Restorative Dentistry, Faculty of Pharmacy, Dentistry and Nursing, Federal University of Ceará, Fortaleza, Ceará, Brazil.
- Graduate Program in Dentistry, Federal University of Ceará, Fortaleza, Ceará, Brazil.
ORCID profiles: Gabriel Freitas Pereira, Maudiela Isabel Arita Torres, Nicole Escórcio de Meneses, Ana Carolina Lima Moreira, Raniel Fernandes Peixoto
Cite
APA
Pereira, G. F., Torres, M. I. A., de Meneses, N. E., Moreira, A. C. L., & Peixoto, R. F. (2026). Influence of Airborne‐Particle Abrasion and Thermal Cycling on Enamel Bond Strength and Roughness of Lithium Disilicate Treated With a Self‐Etching Ceramic Primer. Journal of Esthetic and Restorative Dentistry, 38(7), 1367-1375. https://doi.org/10.1111/jerd.70132
Vancouver
Pereira GF, Torres MIA, de Meneses NE, Moreira ACL, Peixoto RF. Influence of Airborne‐Particle Abrasion and Thermal Cycling on Enamel Bond Strength and Roughness of Lithium Disilicate Treated With a Self‐Etching Ceramic Primer. Journal of Esthetic and Restorative Dentistry. 2026;38(7):1367-1375. doi:10.1111/jerd.70132
BibTeX
@article{Pereira2026,
author = {Pereira, Gabriel Freitas and Torres, Maudiela Isabel Arita and de Meneses, Nicole Escórcio and Moreira, Ana Carolina Lima and Peixoto, Raniel Fernandes},
title = {Influence of Airborne‐Particle Abrasion and Thermal Cycling on Enamel Bond Strength and Roughness of Lithium Disilicate Treated With a Self‐Etching Ceramic Primer},
journal = {Journal of Esthetic and Restorative Dentistry},
year = {2026},
volume = {38},
number = {7},
pages = {1367--1375},
doi = {10.1111/jerd.70132}
}
EUVIMED