Influence of surface treatments and adhesive protocols on repair bond strength of glass‐matrix and resin‐matrix CAD / CAM ceramics
Journal of Esthetic and Restorative Dentistry · 2023-12 · 35 (8) · 1322-1331
DOI: 10.1111/jerd.13131 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Esthetic and Restorative Dentistry, online erschienen am 07.09.2023. Verfasst von Rana Turunç-Oğuzman und 1 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthodontics, Faculty of Dentistry, Altınbaş University, Istanbul, Turkey. Hauptthemen laut MEDLINE: Dental Bonding. Die Arbeit wurde bisher 23-mal zitiert (Crossref) und nennt 42 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
Objective
To specify the effects of self‐etching ceramic primer, Monobond Etch and Prime (MEP), and universal adhesive (UA) on repair bond strength between CAD/CAM blocks and resin composite. Materials and Methods Vita Mark II (VM), IPS e.max CAD (EMAX), Shofu Block HC (SHC), and Tetric CAD (TET) blocks were sliced and thermocycled. They were divided into four groups according to surface treatments ( n = 24): control, sandblasting (AL), hydrofluoric acid etching (HF), and MEP application. SEM analysis assessed surface topography. Subdivided, specimens followed distinct adhesive protocols ( n = 12): control (silane + adhesive [SA] or adhesive [A] only for MEP group) and UA. Microshear bond strength (μSBS) was measured following resin composite repair. Data were analyzed using two‐way ANOVA and Tukey tests ( p < 0.05).
Results
The μSBS of CAD/CAM blocks was significantly influenced by surface treatment type and adhesive protocol. The highest μSBS values for each block, considering surface treatment + adhesive protocol, were VM, HF + SA, or HF + UA; EMAX, MEP + A; and SHC and TET, AL + SA, or AL + UA.
Conclusions
Except for EMAX, it was not the adhesive protocol that made the significant difference in bond strength for each CAD/CAM block, but the surface treatment. MEP + UA application on glass ceramics lowered μSBS values significantly, so it is not recommended in clinical conditions. Clinical Significance Repair is an essential therapeutic option, particularly in esthetic restorations, to swiftly repair the impaired esthetics caused by fracture. Repair protocol is dependent on the restorative material, and to have a reliable repair bond strength, the following surface treatment and adhesive protocol combinations are recommended for each CAD/CAM block: VM, HF + SA, or HF + UA; EMAX, MEP + A; and SHC and TET, AL + SA, or AL + UA.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Department of Prosthodontics, Faculty of Dentistry, Altınbaş University, Istanbul, Turkey.
- Department of Restorative Dentistry, Faculty of Dentistry, Istanbul University-Cerrahpaşa, Istanbul, Turkey.
ORCID-Profile: Rana Turunç-Oğuzman, Soner Şişmanoğlu
Zitieren
APA
Turunç-Oğuzman, R., & Şişmanoğlu, S. (2023). Influence of surface treatments and adhesive protocols on repair bond strength of glass‐matrix and resin‐matrix CAD / CAM ceramics. Journal of Esthetic and Restorative Dentistry, 35(8), 1322-1331. https://doi.org/10.1111/jerd.13131
Vancouver
Turunç-Oğuzman R, Şişmanoğlu S. Influence of surface treatments and adhesive protocols on repair bond strength of glass‐matrix and resin‐matrix CAD / CAM ceramics. Journal of Esthetic and Restorative Dentistry. 2023;35(8):1322-1331. doi:10.1111/jerd.13131
BibTeX
@article{TurunOuzman2023,
author = {Turunç-Oğuzman, Rana and Şişmanoğlu, Soner},
title = {Influence of surface treatments and adhesive protocols on repair bond strength of glass‐matrix and resin‐matrix CAD / CAM ceramics},
journal = {Journal of Esthetic and Restorative Dentistry},
year = {2023},
volume = {35},
number = {8},
pages = {1322--1331},
doi = {10.1111/jerd.13131}
}
EUVIMED