EUVIMEDAtrasti EUVIMED
Crossref

Low‐Temperature Densification of SiC Ceramics With Robust Mechanical Properties Using Si–B 4 C Additive

Bohan Wang, Dengke Zhao, Yiyao Ge, Kexin Chen, Guanghua Liu

Journal of the American Ceramic Society · 2026-11 · 109 (11)

DOI: 10.1111/jace.71422 ↗

At a glance

Journal article in Journal of the American Ceramic Society, published online on 2026-11-10. Written by Bohan Wang and 4 co-authors. 57 references. Funded by: National Natural Science Foundation of China.

SantraukaBibliografiniai duomenysCiteRelated studies

Abstract (original language)

The strong covalent bonding of SiC makes its densification difficult, typically requiring high sintering temperatures. Reaction sintering provides an effective approach to lowering the fabrication temperature of SiC ceramics. In this study, an Si–B 4 C reactive sintering strategy was developed for the low‐temperature densification of SiC ceramics by spark plasma sintering. The effects of the Si–B 4 C additive on the phase evolution, microstructure, and mechanical properties of SiC ceramics were systematically investigated. The role of the Si–B 4 C additive in promoting the low‐temperature densification of SiC ceramics was also elucidated. At a fixed total additive content of 15 wt%, partial replacement of Si with B 4 C substantially accelerated the densification of SiC ceramics during sintering. The average densification rate of the Si–B 4 C additive was substantially higher than that of the Si‐only additive. A nearly dense SiC ceramic was obtained by sintering at 1450°C for 10 min using the Si–B 4 C reactive sintering additive. The low‐temperature densification was attributed to the combined effects of liquid Si and the reaction between Si and B 4 C to form secondary SiC. After sintering at 1500°C for 5 min, SiC ceramics with the Si–B 4 C additive exhibited a Vickers hardness of 29.0 GPa, Young's modulus of 382 GPa, and a fracture toughness of 2.9 MPa m 1/2 . These results demonstrate that Si–B 4 C reactive sintering strategy enables low‐temperature densification of SiC ceramics while retaining robust mechanical properties.

Funding

  • National Natural Science Foundation of China

Cite

APA

Wang, B., Zhao, D., Ge, Y., Chen, K., & Liu, G. (2026). Low‐Temperature Densification of SiC Ceramics With Robust Mechanical Properties Using Si–B 4 C Additive. Journal of the American Ceramic Society, 109(11). https://doi.org/10.1111/jace.71422

Vancouver

Wang B, Zhao D, Ge Y, Chen K, Liu G. Low‐Temperature Densification of SiC Ceramics With Robust Mechanical Properties Using Si–B 4 C Additive. Journal of the American Ceramic Society. 2026;109(11). doi:10.1111/jace.71422

BibTeX
@article{Wang2026,
  author = {Wang, Bohan and Zhao, Dengke and Ge, Yiyao and Chen, Kexin and Liu, Guanghua},
  title = {Low‐Temperature Densification of SiC Ceramics With Robust Mechanical Properties Using Si–B 4 C Additive},
  journal = {Journal of the American Ceramic Society},
  year = {2026},
  volume = {109},
  number = {11},
  doi = {10.1111/jace.71422}
}
Start for free →