Abstract (Originalsprache)
Polyether electrolytes are compelling candidates for lithium metal batteries owing to their high ionic conductivity and conformal interfacial contact. However, their widespread adoption is impeded by inherent vulnerabilities, including limited oxidative stability against high-voltage cathodes, uncontrolled lithium dendrite growth, and persistent interfacial side reactions. To overcome these challenges, we report an in situ polymerized cross-linked polyether electrolyte engineered with a bifluorinated molecular architecture (PTFMO-BEP), incorporating −CF2– segments in the polymer backbone and −CF3 groups on the side chains. This design significantly enhances the intrinsic oxidative stability, extending the electrochemical window beyond 5.5 V. Concurrently, the electron-withdrawing fluorinated motifs weaken the Li+-polymer coordination, steering an anion-derived decomposition pathway to form a homogeneous, inorganic-rich solid electrolyte interphase (SEI). Consequently, the PTFMO-BEP electrolyte enables exceptional cyclability in Li||Li symmetric cells (>800 h) and uniform, dendrite-free lithium deposition. When paired with high-loading LiNi0.8Co0.1Mn0.1O2 (NCM811) cathodes (∼4.4 mAh cm–2) and thin lithium anode (50 μm), the Li||NCM811 full cells achieve outstanding capacity retention of 85.6% after 150 cycles at 4.3 V and 91.5% after 100 cycles at 4.5 V. Remarkably, stable operation is maintained even under an ultrahigh cutoff voltage of 4.7 V with a 20 μm Li anode (88.7% retention over 100 cycles). Furthermore, ampere-hour-scale pouch cells configured with LiNi0.90Co0.05Mn0.05O2 (NCM9055) cathodes deliver a high gravimetric energy density of 510.1 Wh kg–1. This work exemplifies a potent molecular-design strategy to advance polyether electrolytes for practical high-energy-density lithium metal batteries.
Förderung
- Research Grants Council, University Grants Committee
Zitieren
APA
Li, S., Tse, Y. T., Hong, H., Cui, Y., Li, D., Feng, S., Hou, Y., Guo, X., Xiong, Q., Zhang, D., Chen, A., Wang, S., & Zhi, C. (2026). In Situ Polymerized Main/Side-Chain Bifluorinated Cross-Linked Polyether Electrolytes for High-Voltage Lithium Metal Batteries. Journal of the American Chemical Society. https://doi.org/10.1021/jacs.6c08830
Vancouver
Li S, Tse YT, Hong H, Cui Y, Li D, Feng S, et al. In Situ Polymerized Main/Side-Chain Bifluorinated Cross-Linked Polyether Electrolytes for High-Voltage Lithium Metal Batteries. Journal of the American Chemical Society. 2026. doi:10.1021/jacs.6c08830
BibTeX
@article{Li2026,
author = {Li, Shimei and Tse, Yu Tat and Hong, Hu and Cui, Yin and Li, Dedi and Feng, Shuo and Hou, Yue and Guo, Xun and Xiong, Qi and Zhang, Dechao and Chen, Ao and Wang, Shixun and Zhi, Chunyi},
title = {In Situ Polymerized Main/Side-Chain Bifluorinated Cross-Linked Polyether Electrolytes for High-Voltage Lithium Metal Batteries},
journal = {Journal of the American Chemical Society},
year = {2026},
doi = {10.1021/jacs.6c08830}
}
EUVIMED