Polymer-Grafted WS 2 Nanocomposites: from Edge-Site Passivation to Melt-Stable Fused Granular Fabrication

Mirko Maturi iD, Alberto Sanz de Leon iD, Luisa M Valencia, Sergio I Molina, Miriam Herrera

ACS Nano · 2026-05-05 · 20 (17) · 12978-12989

DOI: 10.1021/acsnano.5c22326 ↗

At a glance

Journal article in ACS Nano, published online on 2026-04-21. Written by Mirko Maturi and 4 co-authors. Institution: Dpto. Ciencia de los Materiales, I. M. y Q. I., IMEYMAT, Facultad de Ciencias, Universidad de Cádiz, Campus Río San Pedro, s/n, 11510 Puerto Real, Cá…. Cited 1 times so far (Crossref); 38 references. The full text is freely available (open access, CC BY 4.0). Funded by: Junta de Andaluc?a, Universidad de C?diz.

AbstraktSubjectsBibliografické údajeCiteRelated studies

Abstract (original language)

Layered transition metal dichalcogenides (TMDs) are widely regarded as chemically inert nanofillers in polymer composites. Here, we demonstrate that this assumption fails under melt-processing conditions. We show that pristine WS2 nanopowders act as heterogeneous catalysts for polyester chain scission during melt extrusion, inducing a catastrophic, 10-fold reduction in molecular weight, severe loss of melt viscosity, printing failure, and brittle mechanical behavior at filler loadings as low as 0.2 wt %. To suppress this unexpected catalytic activity, we develop an edge- and defect-selective functionalization strategy for WS2 based on covalent carboxylation and hydroxylation, followed by surface-initiated ring-opening polymerization of ε-caprolactone. Spectroscopic and microscopic analyses (XPS, XRD, HAADF-STEM, and EELS) demonstrate that polymer grafting is confined to edge and defect sites, while preserving the multilayer 2H-WS2 lattice. When incorporated into a polycaprolactone (PCL) matrix and processed by large-format fused granular fabrication, polymer-grafted WS2 nanostructures exhibit stable melt rheology, excellent printability, and substantial mechanical reinforcement, with Young's modulus and tensile strength increases up to 45% and 65%, respectively, without loss of ductility. Crucially, polymer grafting effectively passivates catalytically active WS2 edge and defect sites, preventing melt-induced polymer degradation. These findings provide direct experimental evidence that exposed edge sites in layered nanomaterials can actively catalyze polymer degradation under melt-processing conditions and establish edge-site passivation as a general design principle to mitigate chemically driven polymer degradation in polyester-based systems during melt processing, with the magnitude of the effect depending on the chemical susceptibility of the host polymer.

Subjects

Author keywords

edge-site catalysismelt-processed nanocompositespolymer degradationsurface-initiated polymer graftingtransition metal dichalcogenides

Authors and institutions

  • Dpto. Ciencia de los Materiales, I. M. y Q. I., IMEYMAT, Facultad de Ciencias, Universidad de Cádiz, Campus Río San Pedro, s/n, 11510 Puerto Real, Cádiz, Spain.
  • Instituto de Ciencia de Materiales de Sevilla (CSIC-US), Americo Vespucio 49, Seville 41092, Spain.

ORCID profiles: Mirko Maturi, Alberto Sanz de Leon

Funding

  • Junta de Andaluc?a
  • Universidad de C?diz

Cite

APA

Maturi, M., Sanz de Leon, A., Valencia, L. M., Molina, S. I., & Herrera, M. (2026). Polymer-Grafted WS 2 Nanocomposites: from Edge-Site Passivation to Melt-Stable Fused Granular Fabrication. ACS Nano, 20(17), 12978-12989. https://doi.org/10.1021/acsnano.5c22326

Vancouver

Maturi M, Sanz de Leon A, Valencia LM, Molina SI, Herrera M. Polymer-Grafted WS 2 Nanocomposites: from Edge-Site Passivation to Melt-Stable Fused Granular Fabrication. ACS Nano. 2026;20(17):12978-12989. doi:10.1021/acsnano.5c22326

BibTeX
@article{Maturi2026,
  author = {Maturi, Mirko and Sanz de Leon, Alberto and Valencia, Luisa M and Molina, Sergio I and Herrera, Miriam},
  title = {Polymer-Grafted WS 2 Nanocomposites: from Edge-Site Passivation to Melt-Stable Fused Granular Fabrication},
  journal = {ACS Nano},
  year = {2026},
  volume = {20},
  number = {17},
  pages = {12978--12989},
  doi = {10.1021/acsnano.5c22326}
}
Start for free →