Flexible Thermoelectric Fibers Based on Shear-Aligned MWCNT/PEDOT:PSS Networks for Versatile Applications

Xu Qin, Xueling Zhao, Ruiyi Tian, Haoyu Mo, Jingjing Zhang, Lifei Chen, Huaqing Xie

ACS Applied Polymer Materials · 18.11.2026

DOI: 10.1021/acsapm.6c03530 ↗

Kurz gefasst

Fachartikel in der Zeitschrift ACS Applied Polymer Materials, online erschienen am 18.11.2026. Verfasst von Xu Qin und 6 weiteren Autor:innen. Die Arbeit nennt 40 Literaturangaben. Gefördert von: Shanghai Education Development Foundation, Shanghai Municipal Education Commission, Science and Technology Commission of Shanghai Municipality.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Flexible thermoelectric fibers for wearable applications require balanced electrical performance, mechanical deformability, and continuous processability. Here, MWCNT/PEDOT:PSS composite fibers were fabricated by wet spinning followed by H2SO4 post-treatment. High-shear fibers exhibited an oriented surface texture and scattering anisotropy, while acid treatment reduced PSS-related spectral contributions. Compared with the low-shear samples, high-shear processing increased electrical conductivity and power factor (PF) by 41.5% and 47.6%, respectively. A loading of 20 wt % MWCNTs was selected by considering thermoelectric performance, spinning continuity, and tensile deformability, yielding fibers with a tensile strength of approximately 250 MPa and a fracture strain of approximately 12%. Electrical conductivity reached 1364.2 S·cm–1 after 3 h of acid treatment, whereas the 2 h treatment produced a Seebeck coefficient of 14.1 μV·K–1 and a PF of 21.2 μW·m–1·K–2. Measurements over 1000 bending cycles and 30 days of exposure to air showed modest conductivity changes and relatively stable Seebeck coefficients. The devices demonstrated temperature sensing, respiratory monitoring, and joint-motion monitoring, with a thermal response time of approximately 1.2 s and wrist-mounted open-circuit voltages of approximately 0.33–0.34 mV. A time-division multiplexing (TDM) strategy using alternating zero-current and constant-current measurements provided separate thermoelectric-voltage and resistance-response channels. These results demonstrate a route to flexible thermoelectric fibers that integrate continuous processability, mechanical deformability, and multimodal wearable sensing.

Förderung

  • Shanghai Education Development Foundation
  • Shanghai Municipal Education Commission
  • Science and Technology Commission of Shanghai Municipality
  • Program for Professor of Special Appointment (Eastern Scholar) at Shanghai Institutions of Higher Learning
  • Gaoyuan Discipline of Shanghai-Materials Science and Engineering
  • Shanghai Engineering Research Center of Advanced Thermal Functional Materials

Zitieren

APA

Qin, X., Zhao, X., Tian, R., Mo, H., Zhang, J., Chen, L., & Xie, H. (2026). Flexible Thermoelectric Fibers Based on Shear-Aligned MWCNT/PEDOT:PSS Networks for Versatile Applications. ACS Applied Polymer Materials. https://doi.org/10.1021/acsapm.6c03530

Vancouver

Qin X, Zhao X, Tian R, Mo H, Zhang J, Chen L, et al. Flexible Thermoelectric Fibers Based on Shear-Aligned MWCNT/PEDOT:PSS Networks for Versatile Applications. ACS Applied Polymer Materials. 2026. doi:10.1021/acsapm.6c03530

BibTeX
@article{Qin2026,
  author = {Qin, Xu and Zhao, Xueling and Tian, Ruiyi and Mo, Haoyu and Zhang, Jingjing and Chen, Lifei and Xie, Huaqing},
  title = {Flexible Thermoelectric Fibers Based on Shear-Aligned MWCNT/PEDOT:PSS Networks for Versatile Applications},
  journal = {ACS Applied Polymer Materials},
  year = {2026},
  doi = {10.1021/acsapm.6c03530}
}
Kostenlos starten →