Controlled Anisotropic Wetting by Plasma Treatment for Directed Self-Assembly of High-χ Block Copolymers
ACS Applied Materials & Interfaces · 2024-05-29 · 16 (21) · 27841-27849
DOI: 10.1021/acsami.4c01657 ↗At a glance
Journal article in ACS Applied Materials & Interfaces, published online on 2024-05-17. Written by Achmad Fajar Putranto and 8 co-authors. Institution: CNRS, CEA/LETI Minatec, Laboratoire des Technologies de la Microélectronique (LTM), Université Grenoble Alpes, 38000 Grenoble, France. Cited 11 times so far (Crossref); 50 references. Funded by: Agence Nationale de la Recherche, R?gion Auvergne-Rh?ne-Alpes, French RENATECH network.
Abstract (original language)
The directed self-assembly (DSA) of block copolymers (BCPs) is a promising next-generation lithography technique for high-resolution patterning. However, achieving lithographically applicable BCP organization such as out-of-plane lamellae requires proper tuning of interfacial energies between the BCP domains and the substrate, which remains difficult to address effectively and efficiently with high-χ BCPs. Here, we present the successful generation of anisotropic wetting by plasma treatment on patterned spin-on-carbon (SOC) substrates and its application to the DSA of a high-χ Si-containing material, poly(1,1-dimethylsilacyclobutane)-block-polystyrene (PDMSB-b-PS), with a 9 nm half pitch. Exposing the SOC substrate to different plasma chemistries promotes the vertical alignment of the PDMSB-b-PS lamellae within the trenches. In particular, a patterned substrate treated with HBr/O2 plasma gives both a neutral wetting at the bottom interface and a strong PS-affine wetting at the sidewalls of the SOC trenches to efficiently guide the vertical BCP lamellae. Furthermore, prolonged exposure to HBr/O2 plasma enables an adjustment of the trench width and an increased density of BCP lines on the substrate. Experimental observations are in agreement with a free energy configurational model developed to describe the system. These advances, which could be easily implemented in industry, could contribute to the wider adoption of self-assembly techniques in microelectronics, and beyond to applications such as metasurfaces, surface-enhanced Raman spectroscopy, and sensing technologies.
Subjects
Author keywords
Authors and institutions
- CNRS, CEA/LETI Minatec, Laboratoire des Technologies de la Microélectronique (LTM), Université Grenoble Alpes, 38000 Grenoble, France.
- CNRS, Bordeaux INP, LCPO, UMR 5629, Univ. Bordeaux, F-33600 Pessac, France.
ORCID profiles: Achmad Fajar Putranto, Marc Zelsmann
Funding
- Agence Nationale de la Recherche
- R?gion Auvergne-Rh?ne-Alpes
- French RENATECH network
- BPI France
Cite
APA
Putranto, A. F., Petit-Etienne, C., Cavalaglio, S., Cabannes-Boué, B., Panabiere, M., Forcina, G., Fleury, G., Kogelschatz, M., & Zelsmann, M. (2024). Controlled Anisotropic Wetting by Plasma Treatment for Directed Self-Assembly of High-χ Block Copolymers. ACS Applied Materials & Interfaces, 16(21), 27841-27849. https://doi.org/10.1021/acsami.4c01657
Vancouver
Putranto AF, Petit-Etienne C, Cavalaglio S, Cabannes-Boué B, Panabiere M, Forcina G, et al. Controlled Anisotropic Wetting by Plasma Treatment for Directed Self-Assembly of High-χ Block Copolymers. ACS Applied Materials & Interfaces. 2024;16(21):27841-27849. doi:10.1021/acsami.4c01657
BibTeX
@article{Putranto2024,
author = {Putranto, Achmad Fajar and Petit-Etienne, Camille and Cavalaglio, Sébastien and Cabannes-Boué, Benjamin and Panabiere, Marie and Forcina, Gianluca and Fleury, Guillaume and Kogelschatz, Martin and Zelsmann, Marc},
title = {Controlled Anisotropic Wetting by Plasma Treatment for Directed Self-Assembly of High-χ Block Copolymers},
journal = {ACS Applied Materials & Interfaces},
year = {2024},
volume = {16},
number = {21},
pages = {27841--27849},
doi = {10.1021/acsami.4c01657}
}
EUVIMED