Mechanical behavior of subtractively and additively manufactured zirconia and polyetheretherketone implant abutments after thermomechanical aging
The Journal of Prosthetic Dentistry · 2025
DOI: 10.1016/j.prosdent.2025.05.005 ↗Kurz gefasst
Vergleichsstudie in der Zeitschrift The Journal of Prosthetic Dentistry, 2025. Verfasst von Oguzhan Sari und 2 weiteren Autor:innen. Beteiligte Einrichtung: Graduate Prosthodontist, Çekmeköy Oral and Dental Health Center, Istanbul, Turkey. Hauptthemen laut MEDLINE: Zirconium, Ketones, Polyethylene Glycols, Dental Abutments. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 52 Literaturangaben. Gefördert von: Ataturk University.
Abstract (Originalsprache)
STATEMENT OF PROBLEM: Zirconia and polyetheretherketone (PEEK) implant abutments, manufactured using both subtractive and additive methods, have been introduced. Although the restorative materials could play an important role in the mechanical behavior of implant-supported prostheses, relevant in vitro studies are lacking. PURPOSE: The purpose of this in vitro study was to compare the fracture resistance and failure mode of the 1-piece custom titanium abutment and 2-piece custom zirconia and PEEK abutments (with a titanium base) according to the manufacturing techniques (subtractive and additive). MATERIAL AND METHODS: A maxillary central incisor was simulated for this study. A total of 50 custom abutments were prepared using 3 different abutment materials (titanium, zirconia, and PEEK) and 2 different manufacturing techniques (subtractive and additive) divided into 5 different groups: Group C; control group, premilled titanium abutment, Group SZ; subtractively manufactured zirconia, Group AZ; additively manufactured zirconia, Group SP; subtractively manufactured PEEK, and Group AP; additively manufactured PEEK. Adhesive resin cement was used to cement the custom abutment to the ti-base and cobalt chromium crown to the custom abutment. The specimens were exposed to thermomechanical aging according to the ISO standard 14801. A static force was then applied with a crosshead speed of 1 mm/minute. Failure mode of the specimens was recorded. The fracture resistance values were analyzed with the Kruskal Wallis test, and multiple comparisons were made with the Dunn test (α=.05). RESULTS: The following average fracture resistance values were found (fracture load [N]/bending moment [Ncm]): Group C (711/523), group SP (504/381), group SZ (460/347), group AZ (362/273), and group AP (199/150). The fracture resistance values of the C group were significantly higher than those of the AZ and AP groups (P
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Substanzen
Autor:innen und Institutionen
- Graduate Prosthodontist, Çekmeköy Oral and Dental Health Center, Istanbul, Turkey.
- Assistant Professor, Department of Prosthodontics, Faculty of Dentistry, Atatürk University, Erzurum, Turkey.
- Associate Professor, Department of Prosthodontics, Faculty of Dentistry, Izmir Democracy University, Izmir, Turkey. Electronic address: mgndogdu@gmail.com.
Förderung
- Ataturk University
Zitieren
APA
Sari, O., Sakarya, R. E., & Gundogdu, M. (2025). Mechanical behavior of subtractively and additively manufactured zirconia and polyetheretherketone implant abutments after thermomechanical aging. The Journal of Prosthetic Dentistry. https://doi.org/10.1016/j.prosdent.2025.05.005
Vancouver
Sari O, Sakarya RE, Gundogdu M. Mechanical behavior of subtractively and additively manufactured zirconia and polyetheretherketone implant abutments after thermomechanical aging. The Journal of Prosthetic Dentistry. 2025. doi:10.1016/j.prosdent.2025.05.005
BibTeX
@article{Sari2025,
author = {Sari, Oguzhan and Sakarya, Rüştü Ersoy and Gundogdu, Mustafa},
title = {Mechanical behavior of subtractively and additively manufactured zirconia and polyetheretherketone implant abutments after thermomechanical aging},
journal = {The Journal of Prosthetic Dentistry},
year = {2025},
doi = {10.1016/j.prosdent.2025.05.005}
}
EUVIMED