Bond strength of orthodontic brackets to CAD/CAM ceramics following various surface treatments
Clinical Oral Investigations · 2026
DOI: 10.1007/s00784-026-06784-0 ↗Kurz gefasst
Fachartikel in der Zeitschrift Clinical Oral Investigations, 2026. Verfasst von Gulben Colak und 2 weiteren Autor:innen. Beteiligte Einrichtung: Department of Restorative, Faculty of Dentistry, Süleyman Demirel University, Isparta, Turkey. gulbencolak@sdu.edu.tr. Hauptthemen laut MEDLINE: Ceramics, Computer-Aided Design, Dental Bonding, Dental Porcelain. Die Arbeit nennt 41 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Suleyman Demirel University.
Abstract (Originalsprache)
Objectives
This study evaluated the shear bond strength (SBS) of two types of orthodontic brackets (ceramic and metal) bonded to two CAD/CAM ceramic materials (feldspathic ceramic and lithium disilicate glass-ceramic), each subjected to different surface treatments, and assessed adhesive remnant index (ARI) scores. Materials and methods Sixty-four ceramic discs (1 mm thick; n = 32 per material) were prepared. Surface pretreatments were alumina air abrasion followed by phosphoric acid etching or hydrofluoric acid etching. Each subgroup was bonded with metal or ceramic brackets using a light-cured adhesive. SBS was measured with a universal testing machine, and ARI was assessed under a stereomicroscope. Three-way ANOVA tested the effects of ceramic type, bracket type, and surface treatment (α = 0.05), and chi-square tests compared ARI distributions.
Results
The results demonstrated that the ceramic type significantly influenced SBS ( p = 0.004). Lithium disilicate glass-ceramic exhibited higher SBS values than feldspathic ceramic. Bracket type also had a significant effect on SBS, regardless of ceramic type or surface treatment ( p = 0.001). However, the applied surface treatments did not produce a significant difference in SBS ( p = 0.546); phosphoric acid etching after alumina air abrasion yielded comparable results to hydrofluoric acid etching. ARI scores did not differ significantly among groups, and debonded surfaces showed no gross ceramic damage under stereomicroscopy.
Conclusions
Ceramic type and bracket type significantly affected SBS, whereas surface pretreatment did not under the tested conditions. Clinical relevance Balancing adequate bracket retention with safe debonding is essential for ceramic restorations. Comparable SBS between the two pretreatments and the absence of visible ceramic damage support conservative, clinically oriented conditioning protocols.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Department of Restorative, Faculty of Dentistry, Süleyman Demirel University, Isparta, Turkey. gulbencolak@sdu.edu.tr.
- Department of Orthodontics, Faculty of Dentistry, Süleyman Demirel University, Isparta, Turkey.
- Department of Restorative, Faculty of Dentistry, Süleyman Demirel University, Isparta, Turkey.
Förderung
- Suleyman Demirel University
Zitieren
APA
Colak, G., Albayrak, E., & Ugurlu, M. (2026). Bond strength of orthodontic brackets to CAD/CAM ceramics following various surface treatments. Clinical Oral Investigations. https://doi.org/10.1007/s00784-026-06784-0
Vancouver
Colak G, Albayrak E, Ugurlu M. Bond strength of orthodontic brackets to CAD/CAM ceramics following various surface treatments. Clinical Oral Investigations. 2026. doi:10.1007/s00784-026-06784-0
BibTeX
@article{Colak2026,
author = {Colak, Gulben and Albayrak, Elif and Ugurlu, Muhittin},
title = {Bond strength of orthodontic brackets to CAD/CAM ceramics following various surface treatments},
journal = {Clinical Oral Investigations},
year = {2026},
doi = {10.1007/s00784-026-06784-0}
}
EUVIMED