Comparison of Fracture Resistance of 3D Printed and Milled Zirconia Veneers and Anterior Crowns

Les Kalman iD, Abdulaziz Alhothan iD, Mehrsima Ghavami-Lahiji iD, Akimasa Tsujimoto iD

Clinical and Experimental Dental Research · 2026

DOI: 10.1002/cre2.70440 ↗

Kurz gefasst

Vergleichsstudie in der Zeitschrift Clinical and Experimental Dental Research, 2026. Verfasst von Les Kalman und 3 weiteren Autor:innen. Beteiligte Einrichtung: Schulich School of Medicine & Dentistry, Western University, London, Canada. Hauptthemen laut MEDLINE: Zirconium, Dental Veneers, Crowns, Printing, Three-Dimensional. Die Arbeit nennt 42 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Schulich Dentistry Internal Research.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Objectives

It has recently become possible to prepare monolithic zirconia restorations through 3D printing, in addition to the typical milling technique. In this study, the fracture resistance of anterior crowns and veneers prepared by both techniques was compared. Materials and Methods Digital files were created for the crown and veneer, and restorations were created by milling (BruxZir Esthetic zirconia) and stereolithography 3D printing (LithaCon 3Y 210). The restorations were cemented to resin abutments and subjected to 50,000 thermal cycles before fracture resistance testing, measuring maximum load at fracture. Fracture resistance was evaluated using a universal testing machine. Data were statistically analyzed at a significance level of α = 0.05.

Results

The milled crowns had values of 2318.37 ± 240.91 N, while the printed crowns showed 1988.15 ± 116.14 N ( p = 0.009). The milled veneers had values of 1640.95 ± 173.19 N, and printed veneers of 1325.75 ± 130.71 N ( p = 0.027).

Conclusions

Clinically estimated occlusal forces in the anterior region are under 200 N, and so while printed restorations had significantly lower fracture resistance than milled ones, this was still far higher than the forces the materials are expected to encounter.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

ZirconiumDental VeneersCrownsPrinting, Three-DimensionalDental Prosthesis DesignDental Restoration FailureDental Stress AnalysisHumansMaterials TestingDental MaterialsComputer-Aided Design

Stichwörter der Autor:innen

3D‐printingCAD/CAM millingadditive manufacturinganterior crownsfracture resistanceprosthodonticsrestorative dentistryzirconia

Substanzen

Zirconiumzirconium oxideDental Materials

Autor:innen und Institutionen

  • Schulich School of Medicine & Dentistry, Western University, London, Canada.
  • Department of Dental Health, College of Applied Medical Sciences, King Saud University, Riyadh, Saudi Arabia.
  • Department of Restorative Dentistry, Dental Sciences Research Center, School of Dentistry, Guilan University of Medical Sciences, Rasht, Iran.
  • Department of Operative Dentistry, Aichi Gakuin University School of Dentistry, Nagoya, Japan.
  • Department of Operative Dentistry, University of Iowa College of Dentistry, Iowa City, Iowa, USA.
  • Department of General Dentistry, Creighton University School of Dentistry, Omaha, Nebraska, USA.

ORCID-Profile: Les Kalman, Abdulaziz Alhothan, Mehrsima Ghavami-Lahiji, Akimasa Tsujimoto

Förderung

  • Schulich Dentistry Internal Research

Zitieren

APA

Kalman, L., Alhothan, A., Ghavami-Lahiji, M., & Tsujimoto, A. (2026). Comparison of Fracture Resistance of 3D Printed and Milled Zirconia Veneers and Anterior Crowns. Clinical and Experimental Dental Research. https://doi.org/10.1002/cre2.70440

Vancouver

Kalman L, Alhothan A, Ghavami-Lahiji M, Tsujimoto A. Comparison of Fracture Resistance of 3D Printed and Milled Zirconia Veneers and Anterior Crowns. Clinical and Experimental Dental Research. 2026. doi:10.1002/cre2.70440

BibTeX
@article{Kalman2026,
  author = {Kalman, Les and Alhothan, Abdulaziz and Ghavami-Lahiji, Mehrsima and Tsujimoto, Akimasa},
  title = {Comparison of Fracture Resistance of 3D Printed and Milled Zirconia Veneers and Anterior Crowns},
  journal = {Clinical and Experimental Dental Research},
  year = {2026},
  doi = {10.1002/cre2.70440}
}
Kostenlos starten →